Here you can find knowledge about Solder Wire Manufacturer, including but not limited to usage methods, installation techniques, troubleshooting and more. Focused on SMT soldering processes. If you can't find what you need, please contact us anytime.

How much do you know about the four temperature zone tips for SMT reflow soldering from lead-free solder paste manufacturers?

How much do you know about the four temperature zone tips for SMT reflow soldering from lead-free solder paste manufacturers?

JJYLead-free solder paste manufacturertheSMTThe reflow soldering specification refers to the tempera

Published: 2026-05-12

Are there any hazards of improper operation of lead-free solder paste reflow soldering? -JJY Solder Paste Manufacturer

In the production processLead-free solder pasteWhat problems may occur during reflow soldering opera

Published: 2026-05-12
After the solder paste soldering is completed, the edges are uneven, there are burrs or stains on the surface?

After the solder paste soldering is completed, the edges are uneven, there are burrs or stains on the surface?

If you find that the edges of the solder paste are uneven, there are burrs or stains on the surface

Published: 2026-05-12
A brief Discussion on whether expired solder paste can still be used?

A brief Discussion on whether expired solder paste can still be used?

It is understood that it is in normal useSMTWhen steel mesh is subjected to surface mount technology

Published: 2026-05-12
Industry Research Shows SMT Solder Process Optimization Has Become a Key Direction

Industry Research Shows SMT Solder Process Optimization Has Become a Key Direction

Industry research shows that SMT solder process optimization has become a core lever for production line upgrades at electronics manufacturing enterprises. Multiple leading EMS manufacturers are launching empirical projects in Q1 2026, including dynamic compensation for reflow oven temperature zones, fine-tuning of solder alloy composition, and 3D simulation of stencil apertures. The wettability, void rate, and long-term thermal cycling reliability of SMT solder are emerging as key metrics for process validation.

Published: 2026-05-08
How long can solder paste be left at room temperature before accelerated deterioration occurs?

How long can solder paste be left at room temperature before accelerated deterioration occurs?

Solder paste begins to deteriorate rapidly after being exposed to room temperature for more than 4 hours. This deterioration is significantly accelerated when ambient humidity exceeds 60%RH or temperature exceeds 25℃, as viscosity increases, metal particle settling and flux delamination become markedly more severe, directly impacting the shelf life of the solder paste and printing yield. Production lines must strictly control the time window between taking the solder paste out of cold storage and putting it into use on the machine.

Published: 2026-04-22
Domestic SMT solder brands secure new orders in overseas markets

Domestic SMT solder brands secure new orders in overseas markets

Industry observations indicate that in the fourth quarter of 2025, EMS capacity expansion in Southeast Asia accelerated, with over 140 new SMT placement lines added in Vietnam and Malaysia, of which 67% of production lines explicitly require solder suppliers to hold IATF 16949 automotive electronics compatibility certification and possess localized rapid response capabilities.

Published: 2026-04-19
Optimization of SMT Solder Production Process to Improve Soldering Efficiency and Reliability

Optimization of SMT Solder Production Process to Improve Soldering Efficiency and Reliability

Starting from January 1, 2026, multiple leading SMT solder suppliers, in collaboration with production line process teams, have completed a new round of reflow soldering adaptability optimization. By adjusting the metal powder particle size distribution and flux activity gradient, the cold solder joint rate of SMT solder in 0.3mm pitch CSP package soldering has been reduced to 0.08%.

Published: 2026-04-14
Accelerated Iteration of SMT Solder Technology: Multiple Enterprises Release New Product Solutions

Accelerated Iteration of SMT Solder Technology: Multiple Enterprises Release New Product Solutions

SMT solder technology iteration has accelerated significantly. Starting from January 2026, enterprises including Senju, Shengmao, VTTI, and Yunchuang Precision have collectively released new SMT solder solutions such as low-void-rate lead-free solder paste, high-temperature reflow compatible solder paste, and low-spatter formulations for nitrogen environments. The products focus on three major directions: high reliability, fine-pitch compatibility, and green process compatibility, responding to the stringent requirements for soldering consistency in 5G communication modules, automotive-grade MCUs, and AI server PCBs.

Published: 2026-04-11
Expansion of SMT Solder Application Fields, Significant Rise in Demand for New Energy Equipment

Expansion of SMT Solder Application Fields, Significant Rise in Demand for New Energy Equipment

SMT solder applications are rapidly expanding from traditional consumer electronics to high-reliability scenarios such as photovoltaic inverters, energy storage BMS, and new energy vehicle electronic control systems. Since January 2026, multiple leading solder manufacturers have reported that orders from new energy customers have exceeded 35%. The combined application of lead-free high-temperature alloy solder and low-temperature sintered silver paste has become a key support for production line upgrades.