In soldering work, when faced with the problem of excessive smoke, the key points lie in the following situations. JJY Low-temperature tin wire manufacturer will further analyze:

It is related to the Flux Content and rosin specification. The more Flux there is, the greater the smoke. Different types of rosin have different purities and structures, and thus the smoke they release will also be different.

Low-temperature tin wire

Among fluxes, surfactants can also cause this. However, because the focus differs, the prices of low-temperature tin wire manufacturers may vary. What needs to be emphasized is the soldering effect first, followed by smoke.

It is related to the users. Partners often encounter consumers who, after taking out the Tin wire, directly melt it on the soldering iron tip, generating a considerable amount of smoke. This method of testing smoke is incorrect. The proper approach is to use a smoke box, solder with the same wire diameter and the same length of tin wire, and solder with the same type of soldering iron. Pay attention to which one emits more smoke.

Or consumers solder the same number of points on a PCB circuit board; usually in this situation, partners judge the amount of smoke by the amount of tin wire melted. It is also related to the power of the soldering iron. For the same type of tin wire, the higher-power iron produces more smoke when soldering than the lower-power one.

Shenzhen JJY Industrial Technology Co., LTD has twelve years of product R&D and manufacturing in the field of Solder Wire production, including Solder paste. JJY is a reliable manufacturer of solder wire, specializing in the production and R&D of solder wire, solder wire (low-temperature solder wire), solder rods, Leaded Solder Paste, and related products.

Related Articles

Back to List

Recommended Products

LFP-5RNTT-305 Halogen-Free Lead-Free High-Temperature Solder Paste

LFP-5RNTT-305 Halogen-Free Lead-Free High-Temperature Solder Paste

LFP-JJY5RNTT-305 halogen-free lead-free high-temperature solder paste uses standard Sn96.5Ag3.0Cu0.5

LFP-5RTS-305 Halogen-Free Lead-Free High-Temperature Solder Paste

LFP-5RTS-305 Halogen-Free Lead-Free High-Temperature Solder Paste

LFP-JJY5RTS-305T3 QFN-specific halogen-free, lead-free high-temperature solder paste, made from low-

LFP-5RR-305 Zero-Halogen REACH Lead-Free High-Temperature Solder Paste

LFP-5RR-305 Zero-Halogen REACH Lead-Free High-Temperature Solder Paste

LFP-JJY5RR-305 automotive-lamp-specific halogen-free lead-free high-temperature solder paste, made f