What Problems Will Occur with Solder Paste if the Printing Dwell Time Is Too Long?

In the solder paste printing process, excessively long residence time of solder paste can cause various problems, such as reduced tackiness, slump, and poor soldering. Timely control of solder paste usage time is key to ensuring product quality.

Published: 2026-08-24
The Boom in New Energy Vehicles Drives Demand for Power Device Solder

The Boom in New Energy Vehicles Drives Demand for Power Device Solder

The explosive growth of the new energy vehicle market has driven increased demand for power device solders, with IGBT and SiC module soldering emerging as a new growth driver.

Published: 2026-08-24
Intensifying Competition in the SMT Solder Industry, SMEs Face Pressure to Transform

Intensifying Competition in the SMT Solder Industry, SMEs Face Pressure to Transform

Competition in the SMT solder industry continues to intensify. In early 2026, leading enterprises further squeezed market space through capacity expansion, technology integration and customer binding. Under multiple pressures such as fluctuating raw materials, rising environmental compliance costs and extended certification cycles for high-end products, small and medium-sized manufacturers generally face practical difficulties including lagging production line upgrades and order concentration toward leading players. The SMT solder sector is accelerating its shift from scale competition to a comprehensive contest of process adaptability and supply chain responsiveness.

Published: 2026-08-16
2026 Solder Paste Industry Policy Regulation Tightens, Environmental Protection Laws and Regulations Push Enterprises to Accelerate the R&D and Promotion Process of Halogen-Free and Low-VOCs Products

2026 Solder Paste Industry Policy Regulation Tightens, Environmental Protection Laws and Regulations Push Enterprises to Accelerate the R&D and Promotion Process of Halogen-Free and Low-VOCs Products

In 2026, policy and regulation in the solder paste industry will become increasingly stringent, as environmental laws and regulations push enterprises to accelerate the R&D and promotion of halogen-free and low-VOCs products. As environmental requirements for electronics manufacturing continue to rise globally, solder paste enterprises face greater pressure in optimizing product formulations and upgrading production processes, while new opportunities for technological innovation and sustainable development are also brought to the industry.

Published: 2026-08-03
Solder Technical Standards in SMT Are Gradually Unified, Promoting Cross-Regional Cooperation

Solder Technical Standards in SMT Are Gradually Unified, Promoting Cross-Regional Cooperation

The SMT solder technical standards have achieved substantial collaborative progress in early 2026. IEC/TC91 and SJ/T 11827-2023 have completed alignment on key parameters, covering melting point range, residue ion content, and wettability testing methods. This has increased the mutual recognition rate of materials among the electronic manufacturing clusters in the Yangtze River Delta, Pearl River Delta, and Chengdu-Chongqing region to 76%, significantly reducing the process debugging cycle and incoming material inspection costs for cross-region contract manufacturers.

Published: 2026-07-15
What solder paste is used for QFN chip soldering, and what defects are prone to occur?

What solder paste is used for QFN chip soldering, and what defects are prone to occur?

QFN soldering places extremely high demands on the activity, particle size distribution and metal content of solder paste. It is recommended to use Type 4 or Type 5 rosin-based no-clean solder paste with a metal content of 90.5±0.3%. In actual production lines, improper solder paste selection or mismatched printing parameters can easily lead to typical defects such as solder bridging, open soldering, tombstoning and bottom bridging.

Published: 2026-07-10

Solder bridging between adjacent pins causing short circuits, key prevention for fine-pitch ICs

Bridge is one of the most common and hardest-to-eliminate defects in fine-pitch IC soldering, manifesting as abnormal molten solder connection between adjacent pins that causes short circuits. Production line data from Jia Jinyuan shows that bridges account for over 67% in QFN0.4mm and BGA0.3mm packages, with the root causes concentrated in the combination of solder paste printing misalignment, improper stencil aperture design, and local overshoot of peak reflow soldering temperature.

Published: 2026-06-23
Solder Technology Iteration in SMT Accelerates, Multiple Enterprises Release New-Generation Products

Solder Technology Iteration in SMT Accelerates, Multiple Enterprises Release New-Generation Products

Solder technology iteration in SMT has accelerated significantly. Starting from January 2026, Senju Metal Industry, Shengmao Technology, Indium Corporation, and Loctite China have successively launched new SMT solder products featuring low void rate, high wettability, and halogen-free enhancement, covering packaging scenarios from 01005 to fine-pitch BGA. Some products have passed production line verification by leading EMS manufacturers and entered the small-batch introduction stage.

Published: 2026-06-22
JJY Showcases Full Soldering Materials at NEPCON Thailand 2026

JJY Showcases Full Soldering Materials at NEPCON Thailand 2026

From June 17 to 20, 2026, NEPCON Thailand 2026, hosted by Reed Exhibitions UK, grandly opened at Hall 100, BITEC Bangkok. As Southeast Asia’s most influential annual professional electronics manufactu

Published: 2026-06-18
Expansion of SMT Solder Application Scenarios, Rising Demand in the Automotive Electronics Field

Expansion of SMT Solder Application Scenarios, Rising Demand in the Automotive Electronics Field

As intelligent driving, in-vehicle infotainment systems, and electrified platforms accelerate their deployment, the demand for high-reliability SMT solder in automotive electronics has increased significantly. Starting from January 2026, multiple Tier1 suppliers have included lead-free high-silver solder in their AEC-Q200 certified bill of materials, and the application of SMT solder in automotive-grade PCBA is extending from traditional BCM modules to key components such as ADAS domain controllers, OBC, and BMS.

Published: 2026-06-17

Want to Learn More? Contact Us

Our technical team is always ready to provide professional solder material selection advice and SMT process solutions.