In the electronics industry, the solder that is used more frequently is6040and6337This type of solder has a development history of several decades, and its manufacturing process is also relatively mature and complete. From this, it can be seen that to replace lead-containing solder, some sufficient conditions must be met, Jia JinyuanSolder paste manufacturerLet's analyze what these conditions are?
From the requirements of the electronics industry for soldered components, what needs to be taken into account is the ability to better avoid damaging most of the characteristics of electronic components, which is relatively commonLead-free solderIts melting point should be as close as possible to that of tin-lead eutectic solder. When the melting point is high, the solder will exceed the heat resistance temperature of electronic components, which will affect the reflow soldering furnace.
From this, it can be seen that using solder with a high melting point is not feasible. Secondly, from the perspective of forging performance, it can be related to electronic components,pcbThe coating of the board has relatively good wettability.
From the perspective of product reliability, it is necessary to be able to achieve relatively good spot welding in the industry. The fracture toughness of the solder itself is also very important. When spot welding is required to have heat-resistant characteristics, due to the application of electronic products, the entire process is bound to cause heat generation, which in turn leads to deformation.
Shenzhen JJY brandThe solder paste has gone through many years12Annual research and development of solder paste and solder wireSolder wireManufacturers of solder paste and wire for lead-free solder paste, leaded solder paste, solder rods, lead-free flux paste, etc.
LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste
LFP-JJY8MH-0307T4 is a halogen-free and lead-free high-temperature solder paste launched by JIAJINYUAN/JJY. It adopts Sn99Ag0.3Cu0.7 alloy formula with 4# particle size (20-38μm), features weak activi
LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste
LFP-JJY5RNTT-305T4 is a halogen-free and lead-free high-temperature solder paste developed by JIAJINYUAN/JJY. Formulated with Sn96.5Ag3.0Cu0.5 alloy, it adopts 4# (20-38μm) powder particle size, featu
LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste
LFP-JJY5RQ-305T4 is a halogen-free and lead-free high-temperature solder paste from JIAJINYUAN/JJY. Adopting Sn96.5Ag3.0Cu0.5 alloy composition with 4# particle size, it features high activity, stable