Products

Products

Solder Paste

LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY8MH-0307T4 is a halogen-free and lead-free high-temperature solder paste launched by JIAJINYUAN/JJY. It adopts Sn99Ag0.3Cu0.7 alloy formula with 4# particle size (20-38μm), features weak activi

View Details

LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RNTT-305T4 is a halogen-free and lead-free high-temperature solder paste developed by JIAJINYUAN/JJY. Formulated with Sn96.5Ag3.0Cu0.5 alloy, it adopts 4# (20-38μm) powder particle size, featu

View Details

LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RQ-305T4 is a halogen-free and lead-free high-temperature solder paste from JIAJINYUAN/JJY. Adopting Sn96.5Ag3.0Cu0.5 alloy composition with 4# particle size, it features high activity, stable

View Details
Solder Wire

Solder nickel-chromium plated lead solder wire

This nickel-chromium plated lead solder wire from JIAJINYUAN/JJY adopts Sn63 alloy formula, with a melting point of 183℃ and stable welding performance. It complies with RoHS standard, supports custom

View Details

Solid high-grade leaded solder wire

This is Solid high-grade leaded solder wire from JIAJINYUAN/JJY, made of Sn63/Pb alloy with a low melting point of 183℃. It features excellent weldability for copper and tin-plated copper parts, stabl

View Details

Lead-based solder wire for aluminum welding is environmentally friendly

This JIAJINYUAN/JJY aluminum welding lead-based solder wire adopts Sn63/Pb alloy formula, featuring a low melting point of 183℃, stable welding performance and good environmental compatibility. It sup

View Details
Solder Bar

High-temperature lead-tin strips

High-temperature lead-tin strips from JIAJINYUAN/JJY adopt high-purity Sn99.5 alloy, featuring a stable melting point and excellent weldability. Fully RoHS compliant, suitable for electroplating and s

View Details

There are lead-tin strips Sn/Pb

This Sn/Pb lead-tin strip from JIAJINYUAN/JJY features a melting point of 183℃ and a working temperature of 260~280℃. It supports customized processing, ideal for welding copper parts and tin-plated c

View Details

Lead-tin strip Sn63Pb37

Sn63Pb37 Lead-tin strip from JIAJINYUAN/JJY features a fixed Sn63Pb37 alloy composition with a melting point of 183℃. It supports customized processing, suitable for welding copper parts and tin-plate

View Details