Key Soldering Points for Different PCB Pad Surface Finishing Processes: Gold Plating, Immersion Silver, and OSP

During PCB pad processing, the soldering performance of ENIG, Immersion Silver and OSP processes differs significantly. The ENIG layer is oxidation-resistant but has poor wettability, requiring high-activity solder paste. Immersion Silver is prone to sulfidation discoloration and sensitive to reflow peak temperature. Uneven OSP film thickness can cause local non-wetting. The three processes must be managed differentially in stencil aperture design, reflow profile setting, and incoming material storage conditions.

Published: 2018-04-13
What defects will be caused if the solder paste is opened directly without sufficient warming?

What defects will be caused if the solder paste is opened directly without sufficient warming?

Opening the solder paste container directly without sufficient warm-up will cause abnormal increase in solder paste viscosity, uneven flux precipitation, poor printing release, and increased void rate of solder joints. In severe cases, it will lead to batch defects such as solder bridging, insufficient solder, and cold solder joints. The warm-up of solder paste must strictly follow the requirement of standing at room temperature for 2 to 4 hours. Before opening the solder paste, it is necessary to confirm that the warm-up is sufficient and there is no condensed water on the surface.

Published: 2018-03-26

Anti-oxidation of Pin Dip Soldering Wave Surface, Reducing Continuous Generation of Solder Dross

During the pin dip soldering process, oxidation of the solder bath surface is the main cause of continuous dross generation. Jiajinyuan anti-oxidation flux, through the synergistic effect of dynamic coverage and active ingredients, forms a dense inert film on the solder bath surface, reducing the oxidation rate by more than 70% during pin dip soldering, cutting daily dross production by 1.2kg, significantly extending the cleaning cycle of the solder pot, and stabilizing solder joint wettability.

Published: 2018-03-24

Solder beads most commonly occur on 01005 small components, affecting product insulation reliability

01005 packaged components, with their extremely small pad dimensions and narrow solder paste volume tolerance, are a high-incidence area for solder beads. Residual solder beads can easily cause creeping discharge and breakdown during high-voltage testing, directly threatening the insulation reliability of products. Production line data from Jiajinyuan shows that this type of defect accounts for 68.3% of the total solder bead incidence, requiring coordinated control from three aspects: stencil aperture design, squeegee pressure, and reflow atmosphere.

Published: 2018-02-20

Solder Paste Usage Control for Thick Copper Foil Soldering on Multilayer Boards

To address persistent issues such as uneven solder paste deposition, cold soldering, and solder bridging during thick copper foil soldering on multilayer boards, this paper draws on 20 years of measured data from Jia Jinyuan's production lines, focuses on precise solder paste dosage control methods, and details the matching logic for thick copper solder paste printing parameters, covering key actions such as stencil aperture design, squeegee pressure and speed coordination, and SPI detection threshold setting before reflow soldering.

Published: 2018-02-09

Cold Soldering in Large-Format Thick Copper PCB Production Is a High-Risk Scenario for Cold Soldering

Cold soldering is one of the most stubborn soldering defects in SMT production of large thick copper boards, occurring frequently especially on PCBs with copper thickness ≥2oz and dimensions ≥400mm×300mm. The root cause is that the large heat capacity of the copper substrate and delayed temperature rise lead to insufficient solder paste reflow. In production line tests, Jiajinyuan cold soldering repair paste can reduce the cold soldering defect rate from 1.8% to below 0.3%.

Published: 2018-02-07

Standard for Solder Paste Rewarming and Soldering Defects Caused by Insufficient Rewarming

The standard for solder paste warm-up directly determines printing accuracy and solder joint reliability. Insufficient warm-up will lead to typical soldering defects such as high solder paste viscosity, poor demolding, solder paste collapse, and cold solder joints. Solder paste must strictly follow the 4-hour room temperature warm-up specification before use to avoid batch SMT defects caused by rushed production line launch.

Published: 2018-01-30

Connector Solder Wire and Bar Compatible with Terminal Dip Soldering and Automatic Soldering

Connector solder must balance wettability, residue control, and thermal shock resistance. Jia Jinyuan solder wires and bars can achieve capillary filling within 0.3 seconds in terminal dip soldering, maintain a bridging rate below 0.08% at an automatic soldering track speed of 1.2 m/min, and meet the dual-mode soldering requirements of 0.5mm-pitch FPC connectors and IDC crimp terminals.

Published: 2018-01-17
Is solder paste conductive? Will it cause circuit short circuits?

Is solder paste conductive? Will it cause circuit short circuits?

The solder paste itself is non-conductive; its metallic components are encapsulated by rosin or resin and remain in an insulating state when not melted. However, before reflow soldering, excessive residue, printing misalignment, or incomplete cleaning may still cause circuit short circuits due to ionic residue or solder bead bridging. In actual production lines, over 85% of short circuit problems stem from process control failures rather than the intrinsic conductivity of the solder paste.

Published: 2018-01-14

Cold Solder Joints Have Rough Surfaces and Poor Mechanical Strength, Prone to Fracture Failure

Cold solder joints with rough surfaces, poor mechanical strength, and susceptibility to fracture failure are a high-frequency failure mode in SMT production lines. The root causes are insufficient melting of the solder paste, inadequate flux activity, or low reflow peak temperature. For Jia Jinyuan solder paste on 0.3mm fine-pitch QFN devices, if the reflow peak temperature is below 217°C, batch cold soldering leading to weak solder joints with thrust below 8gf is highly likely to occur.