Solder Paste Alloy Powder

Focused on SMT soldering processes, a one-stop electronic soldering solutions provider.

Solder Paste Alloy Powder
Home Solder Paste Alloy Powder Solder Paste Alloy Powder for Raw Material Ratio, SMT Solder Paste Alloy Powder Raw Material

Solder Paste Alloy Powder for Raw Material Ratio, SMT Solder Paste Alloy Powder Raw Material

Solder Paste Alloy Powder Knowledge

Here you can find knowledge about Solder Paste Alloy Powder, including but not limited to usage methods, installation techniques, troubleshooting and more. Focused on SMT soldering processes. If you can't find what you need, please contact us anytime.

Gold-plated Board Soldering: Common Surface Finish Process for Medical and Precision Instrument PCBs

Gold-plated board soldering undertakes high-reliability connection tasks in the manufacturing of medical and precision instrument PCBs. Its surface process must balance solderability, corrosion resistance, and long-term signal stability. Gold-plated board soldering is particularly suitable for scenarios requiring micro pads, high-frequency devices, and low contact resistance. Gold layer thickness control, nickel barrier integrity, and reflow parameter matching are key bottlenecks for mass production yield.

Published: 2013-06-11
Can Adding Antioxidants to Solder Bars Completely Eliminate Solder Dross Generation?

Can Adding Antioxidants to Solder Bars Completely Eliminate Solder Dross Generation?

Although adding antioxidants to solder bars can significantly delay oxidation reactions and reduce the amount of dross generated during high-temperature molten soldering, it cannot completely eliminate dross formation due to multiple production line variables such as wave soldering temperature fluctuations, flux residue decomposition, molten solder agitation intensity, and alloy composition segregation. There are clear process boundaries for the effectiveness of solder oxidation resistance.

Published: 2013-06-07

Low-Void Solder Paste for High-Frequency Board Soldering to Reduce Fluctuations in Solder Joint Dielectric Parameters

High-frequency board welding is extremely sensitive to solder paste voiding rate. Dielectric parameter fluctuations caused by voids directly degrade signal integrity. Jiajinyuan low-void solder paste, by optimizing metal content, flux volatilization gradient and reflow wetting dynamics, stably controls the voiding rate of BGA solder joints within 3.2% in 5G RF module tests, significantly suppressing insertion loss drift in high frequency bands.

Published: 2013-05-22

Comparison of Wettability Between Halogen-Free Solder Paste and Ordinary Solder Paste

There is a significant difference in solder paste wettability between halogen-free solder paste and ordinary solder paste. The removal of halogen components in halogen-free solder paste leads to a decrease in flux activity, manifested as a 5%~8% reduction in pad spread rate and an approximately 0.12mm decrease in pin climb height. However, its residue has strong insulation and low corrosion risk, making it suitable for high-reliability military and medical electronic production lines.

Published: 2013-05-07

Low-Ion-Residue Sensor Soldering Solder Ensures Stable Sensing Signals

Sensor soldering solder with low ionic residue can significantly suppress leakage current and interfacial electrochemical migration, avoiding sensing signal drift and zero-point offset. Especially in MEMS and gas sensors with high impedance and microvolt-level output, excessive ionic residue will directly lead to deteriorated signal-to-noise ratio and reduced long-term stability. The Jiajinyuan LIS-702 series solder has a measured Cl?+Br?<0.05 wt% and Na?+K?<0.12 wt%, meeting the no-clean grade requirements of IPC J-STD-004B.

Published: 2013-04-29

Nitrogen Reflow: Introducing Nitrogen Protection in Reflow Ovens to Reduce High-Temperature Solder Oxidation

Nitrogen reflow involves introducing high-purity nitrogen into the reflow oven to significantly reduce the oxygen content in the chamber to below 100 ppm, thereby inhibiting the oxidation reaction of metal components such as tin, silver, and copper in the solder paste at high temperatures, improving the brightness and wettability of solder joints, and reducing void rate and cold solder risks. It is a key process method for the stable mass production of Jia Jinyuan series reflow ovens in the soldering of fine-pitch devices such as QFN and BGA.

Published: 2013-04-16

SMT Soldering BGA/QFN Chip Placement: Low-Voidage Solder Paste is Key

When soldering BGA/QFN chips via SMT, an excessive void rate can lead to cold solder joints, increased thermal resistance, and early failure, and low-void solder paste is the core solution to this problem. The void rate of Jiajinyuan JL-808 series solder paste is stably controlled below 8% in mass production. Combined with optimized stencil aperture design and nitrogen-protected reflow, it can reduce the void rate at the bottom of QFN packages from 25% to 6.3%, while the void rate of individual BGA balls is simultaneously reduced to 4.1%.

Published: 2013-03-25
What indicator does the level of tin dross rate in tin wire production represent?

What indicator does the level of tin dross rate in tin wire production represent?

The tin slag rate in solder wire production directly reflects the stability of the smelting process and the level of raw material purity control. An excessively high tin slag rate often indicates intensified oxidation of molten tin, accelerated impurity enrichment, or uncontrolled temperature fluctuations, which can easily lead to batch defects in finished solder wire such as slag inclusions, uneven wire drawing, and reduced wettability.

Published: 2013-03-19

ASEAN Foreign Trade Solder Supports Small-Batch Trial Orders, with Subsequent Stable Large-Volume Delivery

ASEAN foreign trade solder is designed specifically for small and medium-sized export orders, supports small-batch trial orders starting from 5kg, and is paired with JJY's proprietary logistics channels and localized technical response to ensure a first trial production pass rate of over 92%. It can later be seamlessly switched to stable monthly delivery at the 20-ton level, truly addressing the pain points of Southeast Asian customers such as difficult early-stage verification and slow batch switching.

Published: 2013-02-21

Adjustment Scheme for Matching Solder Paste to Offset of Small Component Placement in Solder Paste

To address the persistent production line issues of small component placement offset and solder paste printing mismatch, this paper proposes a practical solution centered on solder paste forming accuracy, with coordinated adjustment of stencil apertures, squeegee parameters, and placement coordinates. It emphasizes the decisive influence of the actual coverage morphology of solder paste on pads on the solder paste positioning tolerance during placement.