What are the advantages and disadvantages of low-temperature lead-free solder paste?
Low-temperature lead-free solder pasteWhat are its advantages? Generally, this kind contains bismuthBiIt's a bit more brittle, made of aluminum substrateLEDHigh-power lamps mostly use low-temperature solder paste, with a melting point of138Products that are not resistant to high temperatures can only use low-temperature solder paste, but the soldering performance of low-temperature solder paste is not as good as that of high-temperature solder paste. The main reason for the application of low-temperature solder paste is that the product design cannot withstand conventional temperature requirements, such asLEDorCOM1thePCB. .
Low-temperature solder paste also has its advantages and disadvantages:
Disadvantage: The low-temperature solder paste isSn-BiAlloys and solder joints are prone to brittle cracking and are not suitable for products with general strength requirements. In addition, when using low-temperature solder paste, components are prone to falling off. Especially for connector products that need to be plugged and unplugged during assembly, they are very likely to fall off.
Advantages: Low-temperature solder paste is relatively cheaper than medium-temperature and high-temperature solder paste because it contains silver, which can reduce costs. Also because of the melting point of low-temperature solder paste138When the temperature of the furnace decreases, the energy consumption will also be reduced..
LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste
LFP-JJY8MH-0307T4 is a halogen-free and lead-free high-temperature solder paste launched by JIAJINYUAN/JJY. It adopts Sn99Ag0.3Cu0.7 alloy formula with 4# particle size (20-38μm), features weak activi
LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste
LFP-JJY5RNTT-305T4 is a halogen-free and lead-free high-temperature solder paste developed by JIAJINYUAN/JJY. Formulated with Sn96.5Ag3.0Cu0.5 alloy, it adopts 4# (20-38μm) powder particle size, featu
LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste
LFP-JJY5RQ-305T4 is a halogen-free and lead-free high-temperature solder paste from JIAJINYUAN/JJY. Adopting Sn96.5Ag3.0Cu0.5 alloy composition with 4# particle size, it features high activity, stable