Reflow Solder Paste

Focused on SMT soldering processes, a one-stop electronic soldering solutions provider.

Reflow Solder Paste
Home Tags Reflow Solder Paste

Reflow Solder Paste for PCBA Process, Temperature-Matched SMT Solder Paste

Reflow Solder Paste Knowledge

Here you can find knowledge about Reflow Solder Paste, including but not limited to usage methods, installation techniques, troubleshooting and more. Focused on SMT soldering processes. If you can't find what you need, please contact us anytime.

Solder Balls Appear in Reflow Solder Paste: Is It a Solder Paste Problem?

Solder Balls Appear in Reflow Solder Paste: Is It a Solder Paste Problem?

The occurrence of solder balling during the reflow soldering process is not necessarily a quality issue with the solder paste itself; it is more often related to the coupling of multiple factors such as printing parameters, stencil design, temperature zone settings, and ambient humidity. Especially when the solder paste is unevenly heated during the reflow stage or the solvent volatilizes insufficiently, splashing-type solder balls are highly likely to be induced. Therefore, troubleshooting should start from the storage conditions of the solder paste, the matching of the reflow soldering profile, and the coordination of the PCB pad layout.

Published: 2024-12-02

Key Application Points of Solder Paste in Vacuum Reflow Soldering Under Formic Acid Atmosphere

In formic acid atmosphere vacuum reflow soldering, solder paste must balance activity control and bubble removal; vacuum solder paste must have low vapor pressure, high thermal stability, and formic acid compatibility, while formic acid reflow solder paste requires a flux system that can synergistically reduce oxides with formic acid without exacerbating metal corrosion. These three factors jointly determine the void fraction and shear strength of solder joints in high-power devices.

Published: 2024-04-21

Adjustment of Solder Paste Process Parameters in Nitrogen Reflow Environment for Solder Paste

Adjusting solder paste process parameters under a nitrogen reflow environment can significantly reduce the solder paste void rate. It is necessary to simultaneously optimize the heating slope, peak temperature and atmospheric oxygen content of reflow soldering, and combine stencil aperture design with squeegee pressure to control printing accuracy, so as to avoid cold solder joints and poor wetting caused by uneven nitrogen displacement or hindered flux volatilization.

Published: 2016-08-11

Solder Paste Soldering Damage Caused by Excessively High Peak Reflow Temperature

Excessively high peak reflow temperature of solder paste will directly lead to excessive growth of intermetallic compounds in solder paste joints, intensified dissolution of pad copper, and thermal damage to component bodies. In actual production lines, common defects include cold solder joints, solder balls, tombstoning, and PCB delamination. This problem mostly stems from inaccurate temperature profile settings, drift of furnace temperature sensors, or uncalibrated differences in activity between different batches of solder paste.

Published: 2015-12-10

Effect of Solder Paste Reflow Soak Zone Duration on Solder Paste Joint Formation

The duration of the constant temperature zone directly affects the synergistic effect of flux activity release and solder joint wetting and spreading in reflow solder paste. If it is too short, it will easily lead to an increase in the void rate of solder paste joints and poor wetting; if it is too long, it will cause excessive growth of intermetallic compounds and thermal damage to components. The actual production line needs to be comprehensively adjusted in combination with the solder paste model, PCB heat capacity distribution, and furnace temperature belt speed.

Published: 2014-08-25

High-Temperature Solder Paste, List of Domestic Solder Paste Brands

This paper focuses on the actual selection logic of high-temperature solder paste among domestic solder paste brands, combining 12 series of parameters verified by first-tier production lines such as Jia Jinyuan, covering QFN solder wetting rate, halogen content, alloy powder type, and the reflow soldering temperature window for solder paste. It particularly emphasizes the stability performance of 0307/305 alloys under the 240–260℃ reflow soldering process for solder paste.

Published: 2009-05-27

Reflow Soldering Paste: Domestic Soldering Paste Tested by Multiple Factories

Multiple factories have tested and confirmed that domestic solder paste performs stably in reflow soldering applications. The 8MQP/5RQ series achieves a solder climbing rate close to 100%, the 8MNTTP/5RNTT series has a halogen content as low as 100~200ppm, and the 8M9P/5RR series delivers 0ppm zero halogen and extremely low voidage. These products cover scenarios including QFN/DFN, automotive lighting, high-precision communications, and ultra-low temperature laser welding. Domestic SMT solder paste replacement now has full temperature range and full process adaptability.

Published: 2009-05-19

High-Activity Solder Paste: Selection Guide for Domestic Solder Paste Brands

The practical performance of high-activity solder paste in achieving nearly 100% solder wetting rate for fine-pitch QFN/DFN devices directly determines the success or failure of domestic solder paste brand selection. Based on the measured data of Jia Jinyuan LFP-JJY series halogen-free and lead-free high-temperature solder paste, this paper compares the differences in residue transparency, halogen content, and alloy powder particle size distribution among models including 8MQP/5RQ, 8MTSP/5RTS, and 8MNTTP/5RNTT in the reflow soldering solder paste process, providing a directly applicable domestic solder paste replacement solution for SMT production lines.

Published: 2009-03-30

Solder Paste Splattering During Reflow: Recommended Reliable Domestic Solder Paste Brands

Solder paste spattering during reflow soldering is mostly caused by printing misalignment, unreasonable stencil aperture design, excessive squeegee pressure, or sudden changes in solder paste viscosity. Selecting anti-spattering solder paste with high thixotropy and low spattering tendency can significantly improve the issue. Domestic solder pastes such as Jiajinyuan LFP-JJY5RNTT-0307 (halogen 100~200ppm) and LFP-JJY5RR-0307 (halogen-free) deliver stable performance in QFN solder wetting rate and void control, making them a cost-effective alternative to imported reflow soldering solder pastes.

Published: 2009-03-26

Post-Soldering Insulation Impedance Meets Standards: Selection of Domestic Solder Paste Brands

Post-welding insulation impedance compliance depends on the ionic cleanliness of solder paste residues and the compactness of the formed film. Domestic high-insulation solder pastes, through strict halogen control (ROL0 grade <500ppm), optimized rosin matrix and T4/T5 fine powder ratio, achieve 70%~100% solder wetting rate for QFN/DFN while ensuring the impedance between reflow solder paste joints is >10^9Ω. Series including LFP-JJY5RNTT, 5RR and 5RLJ have been mass-applied in communication module and automotive LED production lines.

Published: 2009-01-19
1

Want to Learn More? Contact Us

Our technical team is always ready to provide professional solder material selection advice and SMT process solutions.