OSP board soldering is a critical process in SMT production lines that is highly prone to cold solder joints, poor wetting, and pad oxidation failures. It is necessary to optimize stencil aperture design, solder paste selection, reflow profile, and first-article verification process in response to the thermal sensitivity, thin-layer characteristics, and weak adhesion to the copper substrate of the OSP anti-oxidation protective film. Otherwise, even if the placement accuracy meets the standards, batch issues such as dull solder joints, insufficient solder climb height, or abnormal ICT test impedance will occur after reflow.
Published: 2014-11-10The solder used in energy storage modules directly determines the welding reliability of energy storage power supply protection boards and inverters. Jiajinyuan solder exhibits no cracks, low void rate, and an interface IMC thickness controlled at 3.2±0.4μm in 125℃ high-temperature cycle tests, and its wetting and spreading consistency on copper substrates and nickel-plated terminals is superior to that of common industry-standard tin-silver-copper systems.
Published: 2014-10-21The pressure adjustment of the squeegee for solder paste printing directly affects the solder paste forming quality. Excessive pressure will cause solder paste collapse, solder spikes or leakage under the stencil, while insufficient pressure will lead to insufficient solder volume, jagged edges or local missing printing. Combined with the rheological properties of printing solder paste and solder paste parameters such as viscosity, metal content and thixotropic index, on-site fine-tuning within the range of 50~120N is required, while simultaneously observing the stencil rebound status, squeegee trailing marks and pad filling completeness.
Published: 2014-10-12SMT defects are a high-frequency source of failures on production lines. Typical issues such as solder balls, voids, tombstoning, and bridging are directly related to printing accuracy, reflow profile, and component coplanarity. Jia Jinyuan production line data shows that 83% of SMT defects stem from solder paste volume deviation exceeding ±15% or improper matching between stencil apertures and PADs.
Published: 2014-09-14Leveraging its solder ODM R&D capabilities, JJY has developed solder pastes and preformed solder sheets with low voiding rate, zero halogen, and high-temperature reflow resistance for scenarios such as medical equipment, new energy vehicle electronic control, and high-reliability industrial modules. Their solder joint thrust reaches over 85MPa, and the IMC layer thickness is controlled within the range of 1.2~1.8μm, meeting the dual certification requirements of ISO 13485 and AEC-Q200.
Published: 2014-09-13
The oxidation resistance of solder bars and the amount of tin dross generated are highly dependent on the alloy composition. The Sn99.0Ag0.3Cu0.7 eutectic solder bar containing 0.3% silver and 0.7% copper exhibits a 40% improvement in oxide film compactness during wave soldering at 250°C, with a measured tin dross rate 65% lower than that of pure tin. While adding trace amounts of nickel or germanium can refine the grain structure, it tends to cause spattering. Production line verification shows that its overall stability is inferior to that of the classic ternary formulation.
Published: 2014-09-08The duration of the constant temperature zone directly affects the synergistic effect of flux activity release and solder joint wetting and spreading in reflow solder paste. If it is too short, it will easily lead to an increase in the void rate of solder paste joints and poor wetting; if it is too long, it will cause excessive growth of intermetallic compounds and thermal damage to components. The actual production line needs to be comprehensively adjusted in combination with the solder paste model, PCB heat capacity distribution, and furnace temperature belt speed.
Published: 2014-08-25Wave soldering of thick-copper PCBs is prone to solder joint voids, poor wetting, and uneven heat absorption caused by copper thickness. Using Jiajinyuan high-wettability solder bars can significantly improve solder climb height and the consistency of fillet formation, with particularly pronounced process advantages in structures with copper thickness above 2oz, large-area copper foils, and multilayer thick-copper constructions.
Published: 2014-08-25Solder paste thermal cycling testing is a key method for evaluating the fatigue resistance of solder paste joints under repeated temperature changes. By simulating the alternating hot and cold processes in the actual service environment of products, it truly reflects the cracking, delamination and failure trends of different solder pastes under thermal stress, and provides a direct basis for production lines to screen high-reliability solder pastes, optimize reflow profiles and determine batch stability.
Published: 2014-07-30Excess solder is the most easily overlooked yet highly consequential defect in the SMT printing process. Excessive solder paste transfer is directly caused by oversized stencil apertures and improper setting of squeegee angle, pressure, and speed parameters, which in turn triggers cascading issues such as bridging between pads, tombstoning, and post-reflow solder balls. On-site data from JJY shows that when the aperture area ratio exceeds 1.05 and the squeegee pressure is >6.5kg, the incidence of excess solder increases by 3.2 times.