Solder Specifications

Focused on SMT soldering processes, a one-stop electronic soldering solutions provider.

Solder Specifications
Home Solder Specifications Selection Reference Solder Specifications, SMT Wave Hand Soldering Various Solder Spec Charts

Selection Reference Solder Specifications, SMT Wave Hand Soldering Various Solder Spec Charts

Solder Specifications Knowledge

Here you can find knowledge about Solder Specifications, including but not limited to usage methods, installation techniques, troubleshooting and more. Focused on SMT soldering processes. If you can't find what you need, please contact us anytime.

Reference for Lead-containing Solder Paste Sn63Pb37 Reflow Process Parameters

Reference for Lead-containing Solder Paste Sn63Pb37 Reflow Process Parameters

Sn63Pb37 leaded solder paste remains irreplaceable in high-reliability fields such as automotive electronics and industrial control due to its eutectic properties and compatibility with mature processes. Its reflow process parameters are evolving toward narrower windows, higher consistency, and stronger equipment coordination. The driving factors include the domestic reflow soldering temperature control accuracy being improved to ±1.5℃, the Tg value of PCB boards generally rising above 150℃, and the proportion of 0201 and smaller package devices exceeding 38%. Practitioners need to simultaneously upgrade the calibration frequency of reflow profilers, refine the compensation rules for stencil apertures, and establish a batch-specific mapping table between solder paste viscosity and printing speed.

Published: 2026-08-27
How to Select SMT Stencil Thickness for Different Solder Paste Alloys

How to Select SMT Stencil Thickness for Different Solder Paste Alloys

The selection of SMT stencil thickness is shifting from experience-driven to solder paste alloy property adaptation-driven. Lead-free high-melting-point alloys have pushed the proportion of ultra-thin stencils below 0.12mm to 38%, while low-temperature solder paste has shown a 12% increase in collapse rate on 0.15mm stencils in production line measurements. Process engineers need to dynamically adjust stencil thickness based on three key factors: alloy melting point, powder particle size, and flux activity.

Published: 2026-08-27
Wave Soldering Solder Bar Replacement Operation: How to Reduce Solder Dross Generation

Wave Soldering Solder Bar Replacement Operation: How to Reduce Solder Dross Generation

The sharp surge in dross generation during wave soldering solder bar replacement has become a high-frequency pain point on production lines. The industry is shifting from experience-based judgment to data-driven solder pot management, systematically reducing dross by optimizing the solder bar addition rhythm, controlling molten oxygen content, and upgrading the dross scraping frequency logic. This not only reduces material loss rates and downtime frequency, but also forces enterprises to restructure the daily maintenance SOP for soldering pots, with frontline process engineers required to master the synergistic relationship between the trend of solder viscosity changes and the critical point of flux carbonization.

Published: 2026-08-27
Key Points for Halogen-Free Solder Paste SMT Soldering and Reflow Profile Adjustment

Key Points for Halogen-Free Solder Paste SMT Soldering and Reflow Profile Adjustment

Reflow profile adjustment during SMT soldering with halogen-free solder paste is a core factor affecting solder joint reliability and defect rates. Based on 20 years of practical production line experience, this paper directly addresses common high-frequency issues such as solder balls, tombstoning, and poor wetting. Focusing on four key variables—heating rate, soaking time, peak temperature, and cooling rate—it provides immediately actionable parameter fine-tuning solutions and error-prevention guidelines.

Published: 2026-08-27
0201/01005 Micro Components, Solder Paste Printing and Soldering Process

0201/01005 Micro Components, Solder Paste Printing and Soldering Process

01005 components are gaining rapid adoption in high-density PCB assembly, and solder paste printing precision has become a yield bottleneck. The industry is addressing this challenge through stencil aperture optimization, closed-loop control of squeegee pressure, and hierarchical management of solder paste rheological properties, while production lines need to simultaneously upgrade AOI recognition algorithms and operators' microscope re-inspection capabilities.

Published: 2026-08-27
Practical Operation Method of Solder Wire Feeding for Manual Soldering of Multi-Pin Connectors

Practical Operation Method of Solder Wire Feeding for Manual Soldering of Multi-Pin Connectors

Addressing the pain points of high manual soldering costs and high rework rates for multi-pin connectors, this summary focuses on optimizing the practical wire feeding methods for solder wire, and proposes 6 immediately implementable cost-reduction actions, covering key links such as soldering tip selection, flux dosage control, and solder feeding rhythm adjustment. A single action can reduce the manual time for a single solder joint by up to 32%, saving over 1400 hours of rework time annually.

Published: 2026-08-27
SMT Solder Paste Cleaning Process: Distinguishing Between No-Clean and Water-Wash Solder Paste

SMT Solder Paste Cleaning Process: Distinguishing Between No-Clean and Water-Wash Solder Paste

The SMT solder paste cleaning process must be precisely matched to the solder paste type. Although no-clean solder paste is nominally described as requiring no cleaning, the risk of ionic residue still needs to be evaluated in high-reliability scenarios. Water-washable solder paste, by contrast, must be paired with a complete cleaning process such as deionized water spraying, ultrasonic cleaning, or brushing. The two types differ fundamentally in cleaning equipment selection, water quality control, and residue inspection.

Published: 2026-08-27
Reliability of Solder Paste Soldering for Double-Sided SMT with Reflow Soldering Twice

Reliability of Solder Paste Soldering for Double-Sided SMT with Reflow Soldering Twice

In the double-sided mounting process, the solder paste soldering reliability of the second reflow pass is highly dependent on printing accuracy, reflow profile matching, and component heat capacity coordination. Based on measured data from mass production lines, this paper explicitly specifies key parameters including a stencil thickness of 0.12mm, a squeegee pressure of 2.8kg, and a reflow peak temperature of 235℃±2℃, and points out that the risk of re-melting of already soldered components on the A side during the B-side reflow pass is concentrated on resistors and capacitors below 0603 and the bottom pads of QFN packages.

Published: 2026-08-27
SMT Soldering of Thick Copper Boards: Optimization of Solder Paste and Temperature Profile

SMT Soldering of Thick Copper Boards: Optimization of Solder Paste and Temperature Profile

SMT soldering of thick copper boards is prone to cold solder joints and insufficient soldering due to their large heat capacity and delayed temperature rise. Solder paste activity matching and precise control of the reflow temperature profile are required to ensure solder joint reliability. The ramp-up rate in the preheating zone must be controlled between 0.5℃/s and 1.5℃/s, and the peak temperature must meet the component class limits specified in IPC-J-STD-020D. Otherwise, batch failures such as solder balls, tombstoning, and PCB delamination will occur.

Published: 2026-08-27
Wave Soldering Flux Matched with Solder Bar to Improve Solder Joint Glossiness

Wave Soldering Flux Matched with Solder Bar to Improve Solder Joint Glossiness

The compatibility between wave soldering flux and solder bars directly affects solder joint gloss, wetting uniformity, and residue morphology. Based on production line measured data, this paper horizontally compares the combined performance of three types of fluxes—rosin-based, no-clean, and water-soluble—paired with 63/37, 60/40, and SAC305 solder bars respectively. The analysis is conducted from four dimensions: wetting angle variation, solder joint reflectivity, bridging occurrence rate, and cleaning difficulty. It is clarified that for scenarios requiring high gloss, rosin-based flux paired with 63/37 solder bars is preferred, while for high reliability requirements, water-soluble flux paired with SAC305 is favored.

Published: 2026-08-27

Want to Learn More? Contact Us

Our technical team is always ready to provide professional solder material selection advice and SMT process solutions.