Evaluation of Bright Residual Solder Paste for QFN/DFN Medium Solder Wetting Mass Production and LFP-5RTS-0307

Evaluation of Bright Residual Solder Paste for QFN/DFN Medium Solder Wetting Mass Production and LFP-5RTS-0307

LFP?5RTS?0307 translucent residual solder paste demonstrates stable performance in medium solder fillet formation mass production for QFN/DFN packages, offers good process adaptability, and its no-clean feature significantly reduces post-processing costs, making it suitable for high-density electronic manufacturing scenarios.

Published: 2026-08-28
Low-Residue Solder Paste: Material Selection for SMT No-Clean Process

Low-Residue Solder Paste: Material Selection for SMT No-Clean Process

Low-residue solder paste is a key material for enabling SMT no-clean processes. It can control ionic residues below 10.06μg/cm2 NaCl equivalent after reflow soldering, avoiding leakage, corrosion, and CAF failures caused by rosin or organic acid residues. It is especially suitable for high-density, fine-pitch automotive-grade and medical electronics assembly without underfill.

Published: 2026-08-27
No-Clean Solder Paste vs Water-Wash Solder Paste: Comparison for SMT Production Line Selection

No-Clean Solder Paste vs Water-Wash Solder Paste: Comparison for SMT Production Line Selection

The selection of no-clean solder paste and water-washable solder paste in SMT production lines directly determines yield, cost, and delivery rhythm. No-clean solder paste, with advantages such as residue ion content <0.5μg/cm2, eliminating the cleaning process to save 2.3 hours of production capacity per shift, and no need for water-based cleaning equipment investment after reflow, is suitable for high-density fast-turnaround production lines. While water-washable solder paste requires supporting spray cleaning machines and DI water systems, its rosin-based activity is stronger, improving the wetting force on OSP boards and oxidized pads by more than 40%, making it more suitable for high-reliability scenarios such as military industry and automotive electronics.

Published: 2026-08-27
Distinguishing Flux Types for Solder Wire: Rosin, No-Clean, and Water-Soluble

Distinguishing Flux Types for Solder Wire: Rosin, No-Clean, and Water-Soluble

The classification of solder wire flux types must strictly align with the activity grades, halogen content, and residue cleanability requirements for rosin-based, no-clean, and water-soluble fluxes specified in the IPC J-STD-004B standard. Although water-soluble fluxes offer the advantages of high activity and easy cleaning, they carry a risk of chloride ion residue exceeding the 2.5μg/cm2 limit. If the production line fails to implement the deionized water rinsing process specified in IEC 61189-2, it will easily lead to PCBA corrosion failure.

Published: 2026-08-27
No-Clean Solder Paste SMT Soldering: Impact of Residues on Testing

No-Clean Solder Paste SMT Soldering: Impact of Residues on Testing

Although no-clean solder paste eliminates the cleaning process in SMT soldering, post-soldering residues can easily cause poor ICT probe contact, false judgments in flying probe testing, and missed detections in functional testing. Based on production line measured data, this paper proposes 6 actionable cost-reduction measures covering solder paste selection, stencil design, reflow parameters, and test fixture maintenance, which can reduce annual test misjudgment working hours by 1200 hours and reduce false rework costs by 84,000 yuan per plant.

Published: 2026-08-27
SMT Solder Paste Cleaning Process: Distinguishing Between No-Clean and Water-Wash Solder Paste

SMT Solder Paste Cleaning Process: Distinguishing Between No-Clean and Water-Wash Solder Paste

The SMT solder paste cleaning process must be precisely matched to the solder paste type. Although no-clean solder paste is nominally described as requiring no cleaning, the risk of ionic residue still needs to be evaluated in high-reliability scenarios. Water-washable solder paste, by contrast, must be paired with a complete cleaning process such as deionized water spraying, ultrasonic cleaning, or brushing. The two types differ fundamentally in cleaning equipment selection, water quality control, and residue inspection.

Published: 2026-08-27

Halogen-Free No-Clean Solder for Sensor Soldering, Suitable for Medical Sensors

The solder used for Jiajinyuan sensor welding adopts a halogen-free formula design, meets the requirements of the IEC 61249-2-21 standard, has an ionic contamination value of post-welding residue lower than 0.5μg/cm² NaCl equivalent, can pass the high-reliability verification of medical sensors without cleaning, and is especially suitable for low-temperature welding scenarios of tiny heat-sensitive components such as platinum resistors and MEMS pressure cores.

Published: 2025-10-14

Selection of Solder Paste for Excessive Ion Contamination During Solder Paste Soldering

Excessive ion contamination from solder paste soldering directly affects PCBA reliability. It is necessary to control it from the source of solder paste selection, giving priority to low-residue, high-purity no-clean solder paste, and cooperating with standardized solder paste testing procedures to ensure that key indicators such as chloride ions and sodium ions meet the requirements of IPC-J-STD-004B Class L0.

Published: 2023-12-17
High-Stability No-Clean Solder Paste, Compatible with 01005 Micro Components, with Improved Printing Anti-Collapse Performance

High-Stability No-Clean Solder Paste, Compatible with 01005 Micro Components, with Improved Printing Anti-Collapse Performance

Jiajinyuan has launched a high-stability no-clean solder paste, specifically designed for 01005 micro components. By optimizing the alloy powder particle size distribution (T4/T5), rosin-based flux system, and rheological property control, it significantly improves printing anti-slump performance while maintaining halogen-free and lead-free high-temperature characteristics, meeting the high solder climbing rate requirements for QFN/DFN.

Published: 2022-12-14

Insulation Leakage Issue Caused by Flux Residue after Reflow of No-Clean Solder Paste

If excessive flux remains after solder paste reflow soldering, especially between high-density PCBs or fine-pitch components, ionic contamination can easily form, leading to reduced insulation resistance, excessive leakage current, or even short-circuit failures. Although no-clean solder paste is nominally specified as not requiring cleaning, the active components of its flux residue, when coupled with moisture on the board surface, can still significantly degrade surface insulation performance.