TLP-7RTHT-62836804 Leaded Solder Paste

TLP-7RTHT-62836804 Leaded Solder Paste

Brand: JJY TinSolder

Model: TLP-JJY7RTHT-62836804

Alloy Composition: Sn62.8Pb36.8Ag0.4

Particle Size: 4#(20~38um)

Viscosity: 180±20 Pa·S

Activity: ROL0

Melting Point: 181℃

Specification: 500g/bottle

ISO9001/14001

Specifications

Name Parameters
SeriesLeaded solder paste 7MTHT/7RTHT
ApplicationsSpecially for outdoor display scenarios; stable viscosity, long stencil life (key advantage); bright joints; concentrated rosin residue distribution (no display discoloration, uniform ink shade)
Halogen250~400ppm ROL0
Flux TypeRosin type
Alloy Powder62362/62836804/6337/6040 and other alloy powders, T2.5, T3, T4, T5

Product Introduction

TLP-7RTHT-62836804 leaded solder paste is made from standard 62836804 leaded alloy spherical solder powder and is compatible with a range of common leaded alloys including 62362, 62836804, 6337, 6040 and 5545, supporting T2.5, T3, T4 and T5 particle sizes. Paired with the 7MTHT/7RTHT rosin-type flux system in a low-halogen eco formula, the flux has a halogen content of 250~400 ppm, meeting ROL0 grade.

It offers excellent viscosity stability and long stencil life; after reflow, rosin residue is concentrated and evenly distributed with uniform ink shade and no stencil halo, producing bright, full joints. Developed for outdoor displays and automotive displays, it also suits high-precision SMT scenarios such as communication, tablets, laptops and mobile phones, as well as conventional chip-scale mass production. It needs no extra flux, adapts well to ordinary components and slightly oxidized boards, is compatible with traditional leaded SMT printing and reflow processes, and offers wide applicability with stable mass-production yield.

Store refrigerated at 0-10°C; shelf life 6 months.

Item Specification Reference Standard
Viscosity 170±20 Pa·S IPC-TM-650
Solder Ball PASS IPC-TM-650
Printing Durability 10 hours or more
Flux Content (10.5士0.5)%
Copper Mirror Corrosion Test PASS IPC-TM-650
Surface Insulation Resistance - Initial 1.0×1013Ω IPC-TM-650
Surface Insulation Resistance - After Humidity 1.0×1012Ω IPC-TM-650
Spread Rate >90% JIS-Z-3197(1999)
Tack Life 8-16 hours or more
Solder Pit Test Pass IPC-TM-650
Shelf Life (2-10°C) 6 months
Printability T4: good printability with 0.3mm aperture stencils
Solder Powder Main Components (%) Impurity Content (%)
Alloy Sn Pb Ag Fe Bi Al Cd Ni Sb Zn Cu As Hg
Sn62.8Pb36.8Ag0.4 62.8±0.5 Rem 0.4±0.1 ≤0.015 ≤0.025 ≤0.001 ≤0.001 ≤0.010 ≤0.040 ≤0.001 ≤0.020 ≤0.010 ≤0.002

What Makes Our Solder Paste Different

Excellent Printing & Soldering

Stable printing viscosity and tack with excellent formability and up to 100% solder climbing height. Bright, full solder joints effectively solve industry challenges such as cold joints, solder bridging, solder balls, tombstoning, and voids.

Eco-Friendly, Halogen-Free, No-Clean

Certified to multiple environmental SGS standards including RoHS, halogen, and REACH (SVHC). Post-solder residue is transparent and colorless, ROL0 no-clean, with high insulation resistance for safe, reliable performance.

Stable Batches, Worry-Free Use

Advanced production and testing equipment from Germany and Japan, strict ISO9001/ISO14001 quality control, and 21 inspection steps per batch ensure consistent, stable performance over the long term.

Technical Support That Solves Problems

Our experienced engineers provide one-on-one service, free on-site debugging, and better-matched solder paste products, solving soldering process issues on the spot.

Core Product Showcase

A full range of solder paste products to meet diverse process needs

Lead-Free Solder Paste

Lead-Free Eco Solder Paste

hot

SAC305 alloy, wide application range, high soldering reliability — the most widely used eco-friendly solder paste today

Low-Temperature Solder Paste

Low-Temperature Solder Paste

New

Sn42Bi58 alloy with a melting point of 138°C, effectively protecting heat-sensitive components such as FPCs

Leaded Solder Paste

Classic Leaded Solder Paste

Value

Sn63Pb37 eutectic alloy with excellent soldering performance and cost efficiency, ideal for general consumer electronics

*Some tables can be scrolled horizontally to view parameters
Model Application Halogen Type Alloy Powder
Leaded Solder Paste
8MN/7RN
High activity, ideal for QFN/DFN high-climbing scenarios; bright solder joints; 600~750ppm
ROL1
Rosin Type Alloy powder such as 62362/62836804/6337/6040
T2.5, T3, T4
Leaded Solder Paste
7M/7R
Suitable for high-precision and standard scenarios such as communications, tablets, laptops, and phones; bright solder joints; 250~400ppm
ROL0
Rosin Type Alloy powder such as 62362/62836804/6337/6040/5545
T2.5, T3, T4, T5
Leaded Solder Paste
7MTWT/7RTWT
Suitable for high-precision and standard scenarios such as communications, tablets, laptops, and phones; withstands long placement after printing without solder blackening or solder balls; bright solder joints; <500ppm
ROL0
Rosin Type Alloy powder such as 62362/62836804/6337/6040/5545/55X/50X/45X/40X/434314
T2.5, T3, T4, T5
Leaded Solder Paste
7MTHT/7RTHT
Dedicated to outdoor display scenarios; stable viscosity and long stencil life (a standout advantage); bright solder joints; concentrated rosin residue (no screen mottling, even ink color) 250~400ppm
ROL0
Rosin Type Alloy powder such as 62362/62836804/6337/6040
T2.5, T3, T4, T5
Leaded Solder Paste
7MH/7RH
General purpose, transparent and bright residue; especially suitable for white boards such as LED, with strong drying resistance and continuous printing for over 16 hours; solder paste can be stored at room temperature; withstands long placement after printing without solder spattering, especially free of solder balls 250~400ppm
ROL0
Rosin Type Alloy powder such as 62362/62836804/6337/6040/5545/55X/50X/45X/40X/434314
T2.5, T3, T4
Leaded Solder Paste
7ML/7RL
Transparent and bright residue; especially suitable for white boards such as LED, with slightly lower drying resistance, so best for fast-consumption scenarios; can also be used for grooved embedded heat sinks to achieve a low void rate 250~400ppm
ROL0
Rosin Type Alloy powder such as 62362/62836804/6337/6040/5545/55X/50X/45X/40X/434314
T2.5, T3, T4
Leaded Solder Paste
7MF/7RF
Dedicated to silver pads such as silver-plated electronic ceramic components, photovoltaic cells, and light-show glass screens; does not corrode silver pads or cause blackening; 150~350ppm
ROL0
Rosin Type Alloy powder such as 62362/62836804/6337/6040/5545
T2.5, T3, T4
Water-Wash Leaded Solder Paste
3MW9/3RW9
Water-washable, lower cost, excellent printing formability; also suitable for energy-storage battery lead grid soldering; ORH1 Water-Wash Type Alloy powder such as 62362/62836804/6337/6040/5545/5050/4555/4060/3565/3070/2575/2080/1585/1090/595
T2.5, T3, T4
Leaded Solder Paste for Stainless Steel & Aluminum
3MW5/3RW5
For soldering stainless steel and aluminum; can be cleaned with water ORH1 Water-Wash Type Alloy powder such as 62362/62836804/6337/6040/5545/5050/4555/4060/3565/3070/2575/2080/1585/1090/595
T2.5, T3, T4

What Problem Do You Want to Solve?

Targeted solutions for every soldering process challenge

Cold & False Joints

Solder Bridging & Shorts

Solder Ball Spatter

Shift & Tombstoning

Voids & Porosity

Full Solder Climbing

Have other soldering issues? Consult our technical engineers now

Free Technical Consultation

Core Product Features

18 years of craftsmanship — every detail is a promise of quality

1 Strong, Bright, Full Solder Joints

With 18 years of R&D and production experience and a scientifically developed modern process formula, our solder paste is highly compatible with the parts being soldered, producing strong, bright, uniform, full solder joints with no solder balls.

2 Low Residue, No-Clean

An ROL0 no-clean eco-friendly flux was developed, leaving little post-solder residue, offering high insulation resistance, keeping the board clean and corrosion-free, and forming a protective layer that prevents re-oxidation of the substrate.

3 Strong Wetting, Excellent Solder Climbing

An optimized flux formula with trace-element alloy additions, combined with a special process, gives the solder paste high activity that fully wets the pads and achieves a high solder climbing height, effectively eliminating cold and false joints, shifting, tombstoning, solder balls, voids, and other issues during soldering.

4 Stable Printing, Good Release

The solder powder particles are round and uniform in size, with no stringing, sticking, or spattering during printing and no collapse, sticking, or peaks after forming. Viscosity changes little over continuous printing, the paste does not dry out, and tack is well maintained without material loss.

5 Water-Washable with High Cleanliness (water-wash solder paste only)

Post-solder residue dissolves and washes away with pure water (deionized water), leaving no residue behind. Cleanliness is very high, achieving excellent ICT test performance without damaging electronic components. The production and cleaning processes generate no pollution and meet environmental requirements. Cleaning is fast — much faster than with other types of solder paste.

Instructions for Use

Follow the guidelines to get the best performance

Storage

Refrigerate at 0-10°C; shelf life 6 months

Warming Up

Take out 2-4 hours before use to reach room temperature

Stirring

Stir thoroughly for 1-3 minutes until uniform

Precautions

Seal and refrigerate any unused solder paste separately

Enterprise Certifications & Advantages

Multiple authoritative certifications, quality you can trust

ISO9001/ISO14001

Quality Management System

SGS Certified

ROHS Compliant

REACH Certified

EU Environmental Certification

Own Brand

18-Year Factory Brand

17+ Certifications
17+ Certifications
18+

Years in Industry

5000+

Customers

21

Inspection Steps

ISO

Quality Certifications

Professional R&D Team

Professional R&D Team · Custom Solutions

Our professional technical team provides custom formulas based on your process requirements. Solder alloys, flux activity levels, cleaning methods and special performance characteristics can all be customized. We also offer product selection advice, optimize soldering processes and provide suitable solutions to improve your first-pass yield.

Strict Quality Control

Strict Quality Control · Stable Performance

A 5000㎡ factory equipped with 96 production and testing machines. ISO9001/ISO14001 certified and strictly implemented. 21 inspection steps ensure stable solder performance. Incoming material, in-process and finished product testing ensure compliance. All eco-friendly products are SGS tested and meet RoHS, halogen-free and REACH (SVHC) standards.

18 Years in Industry

18 Years of Experience · Excellent Soldering Results

18 years focused on solder paste R&D and production. Using high-purity virgin tin, optimized flux formulas and a special process that adds trace-element alloys. Our solder paste precisely matches assembly scenarios, delivering fast climbing and bright, full solder joints. No cold joints, bridging, solder balls, tombstones, voids, stringing, slump or drying issues. Factory-direct sales with no middlemen for better value.

Real-Time Technical Support

Real-Time Technical Support · On-Site Service

Senior engineers provide pre-sales consulting and after-sales technical support with one-on-one service. Free on-site debugging and product matching. On-site problem solving. Solutions provided within 24 hours and issues resolved within 72 hours. Free replacement for quality issues.

Advanced Production & Testing Equipment

High-end equipment from Germany and Japan ensures product precision and quality

Vacuum Mixing (Tank and Syringe) Batch Filling Integrated Machine (1)

Vacuum Mixing (Tank and Syringe) Batch Filling Integrated Machine (1)

German SPECTRO Spectroscopy Analyzer

German SPECTRO Spectroscopy Analyzer

Japanese Malcom solder paste viscosity meter

Japanese Malcom solder paste viscosity meter

Solder paste dispensing and spraying + Laser welding testing machine

Solder paste dispensing and spraying + Laser welding testing machine

Our Clients

Serving many well-known enterprises, trusted by customers

ECOVACS
TwoWing
Thyssenkrupp
Sanrui
NARI
INT
KONKA
HENDERA

Inquire Now for Exclusive Offers

Free samples + on-site debugging by technical engineers

Call Us: +86 0755-88366766

WeChat Support

WeChat Support QR Code

Scan to add us on WeChat