Wave soldering is mainly used for making soldering software, while reflow soldering is used for making surface mount components. So will there be any other differences between them? Shenzhen JJYSolder paste manufacturerLet's answer for our partners:

Solder paste manufacturer

Wave soldering is carried out after meltingSolderingThe formed solder wave peaks are then used to solder the components. On the contrary, reflow soldering takes place in the hot air of a high-temperature area, where the solder is reflow and melted, and only then can the soldering work of components be carried out.

The working processes of wave soldering and reflow soldering are different.

Wave soldering, it isGet it done.After applying the flux, it can enter the preheating area and then proceed to wave soldering for further welding. After welding, the edges and corners must be removed and the defects of the welded products should be inspected. A complete wave soldering can be divided into four major modules, namely "spray, preheating zone, soldering furnace, and cooling zone".

Reflow soldering is done firstDo wellSolder pasteAfter the printing is completed and the components are properly mounted, it can enter the reflow soldering process for soldering. Then, a cleaning and washing operation should be carried out on the soldered products. A complete reflow soldering can be divided into three major area modules, namely "preheating, heating, and cooling".

Shenzhen JJYThe brand's solder paste is suitable for your choice. We offer a solution tailored to your needs. For solder paste manufacturers, choose JJY. Welcome partners to come and consult about other soldering products such as solder wire, solder bar, solder wire, wave solder bar, lead-free solder paste, red glue, etc.

Related Articles

Recommended Products

LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY8MH-0307T4 is a halogen-free and lead-free high-temperature solder paste launched by JIAJINYUAN/JJY. It adopts Sn99Ag0.3Cu0.7 alloy formula with 4# particle size (20-38μm), features weak activi

View Details
LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RNTT-305T4 is a halogen-free and lead-free high-temperature solder paste developed by JIAJINYUAN/JJY. Formulated with Sn96.5Ag3.0Cu0.5 alloy, it adopts 4# (20-38μm) powder particle size, featu

View Details
LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RQ-305T4 is a halogen-free and lead-free high-temperature solder paste from JIAJINYUAN/JJY. Adopting Sn96.5Ag3.0Cu0.5 alloy composition with 4# particle size, it features high activity, stable

View Details