Focused on SMT soldering processes, a one-stop electronic soldering solutions provider.
Here you can find knowledge about Solder Paste Flux, including but not limited to usage methods, installation techniques, troubleshooting and more. Focused on SMT soldering processes. If you can't find what you need, please contact us anytime.
The post-soldering corrosion risk of SMT solder paste is highly dependent on the chemical composition of the solder paste flux. Different systems, such as rosin-based, water-soluble, and no-clean, exhibit significant differences in ionic residue, halogen content, and activation temperature. The probability of post-soldering corrosion increases notably when the chloride ion concentration exceeds 0.5μg/cm2, the softening point of rosin resin is below 120℃, or the pKa value of organic acids is less than 4.2.
Published: 2026-08-27After reflow soldering, solder joints turn black, which is mainly related to flux residues in the solder paste. By controlling solder paste usage, optimizing reflow soldering parameters, and strengthening the cleaning process, residue problems can be effectively reduced and soldering quality can be improved.
Published: 2026-08-24Unstable soldering quality of OSP boards often stems from a mismatch between the activity of solder paste flux and the chemical stability of the OSP film, leading to poor wetting, cold solder joints, or blackened solder joints. Jiajinyuan series solder paste precisely removes the OSP film without corroding the copper surface through a gradient activity design, and its controllable stripping capability for 0.3μm thick OSP film has been verified on multiple production lines.
Published: 2025-09-27For the typical solder paste defect of solder paste flux splatter contaminating PCBs, actionable improvement countermeasures that can be implemented immediately are proposed from four aspects: solder paste selection, stencil aperture design, printing parameter matching, and pre-reflow standing control. The synergistic matching of solder paste flux activity and viscosity is emphasized, avoiding reliance solely on cleaning or process compromises.
Published: 2024-01-16If excessive flux remains after solder paste reflow soldering, especially between high-density PCBs or fine-pitch components, ionic contamination can easily form, leading to reduced insulation resistance, excessive leakage current, or even short-circuit failures. Although no-clean solder paste is nominally specified as not requiring cleaning, the active components of its flux residue, when coupled with moisture on the board surface, can still significantly degrade surface insulation performance.
Published: 2021-08-28Insufficient flux activity in solder paste will significantly weaken its ability to remove oxide films, leading to poor pad wetting after solder paste printing and insufficient solder spreading during reflow, which ultimately causes cold solder joints in the solder paste. This issue is particularly prominent in 0201/01005 micro components, OSP surface-treated PCBs, and low-temperature reflow processes, requiring coordinated verification from three aspects: flux acid value, halogen content, and activation temperature window.
Published: 2020-09-21The volatilization rate of solder paste flux directly affects the wettability, void rate, and bridging risk of solder paste joints. Excessively fast volatilization can easily lead to insufficient solder paste collapse and cold solder joints, while excessively slow volatilization leaves residual flux that causes splashing and solder balls. Based on 20 years of practical SMT production line data from Jiajinyuan, this paper analyzes the cascading impact of the actual volatilization behavior of solder paste flux under different temperature zone settings on the formation of solder paste joints.
Published: 2011-07-15Our technical team is always ready to provide professional solder material selection advice and SMT process solutions.