Solder Procurement Knowledge

Here you can find knowledge about Solder Procurement, including but not limited to usage methods, installation techniques, troubleshooting and more. Focused on SMT soldering processes. If you can't find what you need, please contact us anytime.

What Production Defects Will Be Caused by Too High or Too Low Solder Paste Viscosity?

What Production Defects Will Be Caused by Too High or Too Low Solder Paste Viscosity?

Abnormal solder paste viscosity directly leads to high-frequency production line defects such as printing defects, component placement misalignment, and reflow voids. Excessively high solder paste viscosity easily causes printing skipping and stencil clogging, while excessively low viscosity leads to slump, bridging, and solder balls. During actual debugging, dynamic adjustments must be made in combination with ambient temperature and humidity, squeegee parameters, and batch differences of solder paste.

Published: 2019-04-28

BGA Soldering on Thick Copper Boards and Multilayer Boards: Large Thermal Capacity Requires Adjustment of Heating Parameters

When soldering thick copper PCBs and multilayer boards with BGA, the significantly increased thermal capacity means conventional heating parameters can easily cause cold solder joints or chip warpage. It is necessary to specifically extend the preheating time, increase the temperature of the soaking zone, and slow down the peak heating slope to ensure synchronous melting of solder balls and overall thermal balance of the PCB.

Published: 2019-04-12

Solder Paste Incoming Inspection Items and Solder Paste Quality Judgment Standards

Incoming solder paste inspection is the first line of defense for SMT process stability. It quickly screens incoming solder paste through key items such as viscosity, metal content, particle size distribution, slump resistance, and wettability, and comprehensively determines solder paste quality by combining printability, reflow performance, and solder joint morphology under a microscope, ensuring that each batch of incoming solder paste meets the production line's process window requirements.

Published: 2019-03-08
What Are the Causes of Solder Bridge Short Circuit During Solder Wire Soldering?

What Are the Causes of Solder Bridge Short Circuit During Solder Wire Soldering?

In solder wire soldering, solder bridges causing short circuits are mostly caused by excessively small pad spacing, mismatch between solder wire diameter and soldering iron temperature, insufficient flux activity, or uncleared residual oxide layers. In actual production lines, 80% of solder bridge problems stem from the imbalance between operating technique and material adaptability, rather than simple deviations in process parameters.

Published: 2019-02-15

Explanation on Batch Traceability of Solder Paste RoHS, REACH, Halogen and SGS Reports

The compliance of solder paste with RoHS, REACH, and halogen regulations directly affects the market access of exported products. SGS solder paste inspection reports must strictly correspond to each batch of physical solder paste. Jia Jinyuan's production line achieves 100% traceability through double-person verification of batch numbers, inspection dates, and consistency with the inkjet codes on solder paste cans, along with synchronized archiving of electronic versions of original SGS solder paste inspection reports, to avoid returning entire batches of PCBA due to mismatched reports.

Published: 2019-02-14

Causes of Solder Paste Component Shift After Long-Term Placement Following Solder Paste Mounting

Prolonged standing after solder paste placement causing solder paste displacement is a high-frequency abnormality on SMT production lines. The root cause lies in the continuous collapse and wetting spreading of the placement solder paste at room temperature, compounded by multiple factors such as component self-weight, vibration disturbance, and PCB micro-warpage deformation, which gradually causes the solder paste on the pads to lose its anchoring force on the components.

Published: 2019-01-24
In 2018, a trend of solder paste formula optimization emerged in the electronics manufacturing industry, and enterprises began to focus on the application scenarios of environmentally friendly and low-residue solder pastes.

In 2018, a trend of solder paste formula optimization emerged in the electronics manufacturing industry, and enterprises began to focus on the application scenarios of environmentally friendly and low-residue solder pastes.

In 2018, a trend of solder paste formula optimization emerged in the electronics manufacturing industry, and enterprises began to pay attention to the application scenarios of environmentally friendly and low-residue solder pastes. With increasingly strict environmental regulations and rising industry demand for high-precision manufacturing, solder paste technology is gradually developing in the direction of low harmful substances and high stability.

Published: 2019-01-01

PCBA Reliability Test Thermal Cycling Test: Verifying the Fatigue Resistance of Solder Joints

Thermal cycling testing is a key method for PCBA reliability testing. Through harsh conditions of -40℃ to +125℃, temperature rise and fall completed within 5 minutes, and a 15-minute dwell per cycle, it simulates temperature stress changes of products in real environments, focuses on exposing microcracks in solder joints and fatigue failure of the IMC layer, and directly reflects the impact of SMT placement processes and reflow profiles on long-term service life.

Published: 2018-12-26

Hand Soldering Mobile Phone Motherboards: Fine-Diameter Solder Wire for Micro Solder Joints

When manually soldering mobile phone motherboards, thin-diameter solder wire can precisely cover pads below 0.3mm, avoiding bridging and cold solder joints. Combined with a constant-temperature soldering iron and a high-magnification microscope, it enables reliable connections of tiny solder joints such as peripheral resistors and capacitors around BGA and cable interfaces, making it an indispensable practical process for rework production lines to handle high-density PCBs.

Published: 2018-12-11

Improvement Solutions for Solder Paste Edge Collapse in Thick Stencil Printing

Aiming at the common edge collapse problem in solder paste printing for thick boards, this paper starts with the collaborative optimization of solder paste rheological properties, stencil aperture design and squeegee parameters, proposes a solder paste selection standard for thick boards adapted to PCB thicknesses above 0.8mm and a tightening scheme for the solder paste printing process window, and emphasizes that yield improvement can be achieved through solder paste viscosity gradient matching and fine-tuning of the standing time before reflow without replacing equipment.

Published: 2018-11-19