專業電子焊接材料在地化供應,錫膏、焊錫絲、焊條一站式採購解決方案,並提供樣品試用和技術支援。
We are a solder paste manufacturing factory based in Shenzhen, China, supplying directly to electronics assembly facilities located in SingaporeTuas Industrial Estate. Our production capability covers the full spectrum of soldering materials including solder paste, solder wire and solder bar — all tailored to meet the process requirements of modern SMT lines.
A local electronics contract manufacturer in SingaporeTuas Industrial Estate previously experienced frequent bridging and cold solder joints using imported solder paste. After switching to our lead-free solder paste formulation with optimized metal content and rheology, they achieved improved print definition and reflow consistency across QFN and fine-pitch components without requiring line stoppages.
For high-reliability applications such as automotive-grade PCB assembly within the estate, we supply medium-temperature solder paste compatible with copper-nickel-gold surface finishes, alongside matching solder wire and solder bar for selective and hand-soldering operations. These materials are delivered in constant-temperature packaging to preserve stability during Singapore’s tropical climate conditions.
Our Shenzhen facility maintains inventory of standard solder paste variants, enabling same-week dispatch to SingaporeTuas Industrial Estate via dedicated courier partnerships. Technical engineers provide remote SMT process support including stencil design review, reflow profile optimization and defect root-cause analysis — ensuring seamless integration into existing production workflows.