News
常问问题

无铅锡条在使用过程中应设定多少温度?

一般来说,在使用过程中,我们应该设定合适的温度。相信很多技术专家都讨论过这个问题。 The general temperature setting for lead-free solder strip soldering is280Positive or negative10The temperature setting is generally high because manual dip welding does not involve preheating,The main components of commonly used eco-friendly tin strips are99.3%Tin0.7%Composed of copper, solid, silvery white and odorless, with a melting point of227℃ The working temperature is270℃-300℃The weld points are relatively bright and are used for welding with higher requirements.广泛应用于波炉和手持式浸入炉。 Environmental-friendly tin strip temperature (peak temperature)270~300℃The specific lead-containing solder rods depend on the lead content and the material of the components to be soldered.下面我们就从JJY锡膏厂家来说说:

Lead-free tin bar

高温锡带:
  液相线温度高于锡铅共晶的熔点。 183℃并可超过450℃能保持其工作温度而不氧化并能正常焊接的锡条称为高温锡条。高温锡条是在锡铅合金中加入特殊配方的添加剂制成的,在超过450℃以上还可以起到氧化作用。该产品适用于工作温度要求较高的焊接工艺。例如:变压器引脚上锡等。我厂备有各种合金配比供客户选择。 

低温锡条
  熔点低于183℃焊料可提供不同的焊接工艺和不同熔点的焊料合金。 

高抗氧化焊锡条
  在300℃以下的焊接温度下,液态能量焊料表面如镜面,润湿时间短,膨胀率比普通焊料大。抗氧化剂的添加使焊点光亮、有光泽、美观,适用于PCB波峰焊和热浸焊。我厂备有各种合金配比供客户选择。 
抗氧化高温焊条
  在450℃高温条件下,焊料表面能长期保持银白色镜面状态,焊渣产量仅为普通焊料的1/7,适用于波峰焊和热浸焊工艺,特别适用于各种变压器制造过程中的自溶漆包线镀锡。低渣含量的效果不仅可以减少有缺陷的焊点并节省成本支出,而且还可以减少焊接的维护机会。

以上就是给大家介绍一下不必要的无铅锡条如果你还想进一步了解各种温度条件,可以一起讨论。


相关文章

推荐产品

LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY8MH-0307T4 无卤无铅高温锡膏

LFP-JJY8MH-0307T4是嘉金源/金晶源推出的一款无卤无铅高温锡膏。采用Sn99Ag0.3Cu0.7合金配方,4#粒径(20-38μm),活性弱。

查看详情
LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RNTT-305T4无卤无铅高温锡膏

LFP-JJY5RNTT-305T4是嘉金源/金晶源开发的一款无卤无铅高温锡膏。采用Sn96.5Ag3.0Cu0.5合金配方,采用4#(20-38μm)粉末粒度,特点

查看详情
LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RQ-305T4无卤无铅高温锡膏

LFP-JJY5RQ-305T4是JIAJINYUAN/JJY的无卤无铅高温焊膏。采用4#粒度的Sn96.5Ag3.0Cu0.5合金成分,具有活性高、稳定性好等特点