Is there any difference between a syringe and canned solder paste? JJY Solder Paste Manufacturer

According to the application scenarios of solder paste, it can be classifiedSyringe-shaped solder pasteAnd bottled solder paste (also known as canned solder paste), used forSMTFor printing, choose bottled solder paste. When it comes to automatic dispensing machine processing, choose syringe solder paste. JJYSolder paste manufacturerLead your friends and explore together what the differences are between them?

Solder paste manufacturer

The secret recipes of the ingredients among them are different, and the actual operations when applying them will also be different. In addition, the two cannot be interchanged when they are welded. Otherwise, the quality of the welding will be relatively poor, such as solder flying or poor welding and other undesirable phenomena.

Syringe typeSolder pasteIt is relatively fine in powder form, the same as canned solder paste. The needle-type solder paste, on the other hand, is soldered with a relatively small solder dot spacing.

Under normal circumstancesSMTSyringe solder paste cannot be used. Because the viscosity of the syringe solder paste is different from that of the canned printed solder paste, and the properties of the solder paste are also different, in the case of soldering, it will increase the occurrence of solder flying and poor soldering. After the syringe solder paste is taken out of the ice zone, it can be stored at room temperature for a period of time and does not need to be placed in a constant temperature device.

Shenzhen JJY Industrial Technology Co., LTDIt is a company that has been engaged in the research of solder paste and solder wire for more than ten years.Solder wireJJY, a manufacturer of solder paste and wire for syringes, lead-free solder paste, leaded solder paste, solder rods, etc., welcomes inquiries from partners.

Related Articles

Recommended Products

LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY8MH-0307T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY8MH-0307T4 is a halogen-free and lead-free high-temperature solder paste launched by JIAJINYUAN/JJY. It adopts Sn99Ag0.3Cu0.7 alloy formula with 4# particle size (20-38μm), features weak activi

View Details
LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RNTT-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RNTT-305T4 is a halogen-free and lead-free high-temperature solder paste developed by JIAJINYUAN/JJY. Formulated with Sn96.5Ag3.0Cu0.5 alloy, it adopts 4# (20-38μm) powder particle size, featu

View Details
LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RQ-305T4 halogen-free and lead-free high-temperature solder paste

LFP-JJY5RQ-305T4 is a halogen-free and lead-free high-temperature solder paste from JIAJINYUAN/JJY. Adopting Sn96.5Ag3.0Cu0.5 alloy composition with 4# particle size, it features high activity, stable

View Details