Halogen-Free Lead-Free High-Temp Solder Paste 8MQP/5RQ |
Mataas na aktibidad, pinakamataas na solder climbing (malapit sa 100%) para sa QFN/DFN at mga katulad na application |
Single<900ppm / Dual<1500ppm ROL1 |
Uri ng Rosin |
Alloy powder tulad ng 0307/105/305 T3, T4, T5 |
Halogen-Free Lead-Free High-Temp Solder Paste 8MTSP/5RTS |
Mas mataas na aktibidad, mahusay na solder climbing (70%-90%) para sa QFN/DFN at mga katulad na aplikasyon; mababa, maliwanag na nalalabi; |
<500ppm ROL0 |
Uri ng Rosin |
Alloy powder tulad ng 0307/105/305 T3, T4, T5 |
Halogen-Free Lead-Free High-Temp Solder Paste 8MNTTP/5RNTT |
Angkop lalo na para sa mga application na may mataas na katumpakan gaya ng mga komunikasyon, tablet, laptop, mobile phone, Bluetooth, at mga lock ng fingerprint; mababa, transparent na nalalabi; |
100~200ppm ROL0 |
Uri ng Rosin |
Alloy powder gaya ng 0307/105/305/00507BN/00507B2N T3, T4, T5 |
Zero-Halogen at REACH Lead-Free High-Temp 8M9P/5RR |
Zero halogen, napakababang void rate, na angkop para sa low-void, high-thermal-conductivity applications gaya ng automotive lighting; mababa, transparent na nalalabi; |
0ppm ROL0 |
Uri ng Rosin |
Alloy powder tulad ng 0307/105/305 T3, T4, T5 |
Halogen-Free Lead-Free High-Temp Solder Paste 8MA |
Angkop para sa pangkalahatan at mas malawak na pitch na karaniwang mga senaryo tulad ng mga lighting LED; mababa, transparent na nalalabi; |
<900ppm ROL1 |
Uri ng Rosin |
0307/0107/SC07/00507BN/00507B2N haluang metal na pulbos T3, T4 |
Karaniwang Halogen-Free Lead-Free Medium-Temp&Low-Temp Solder Paste 8M/2R (8MTHL/2RTHL) |
Para sa mga senaryo na walang lead na medium-temp at low-temp na kinukunsinti lang ang katamtaman/mababang temperatura, gaya ng mga LED, crystal oscillator, copper wire na ilaw, at transparent na screen; |
800~900ppm ROL1 |
Uri ng Rosin |
Sn64Bi35Ag1/Sn64.7Bi35Ag0.3/Sn42Bi58/Sn42Bi57Ag1/Sn49.6Bi48.5Ag1Cu0.9/high-reliability LT32S alloy powder T2.5, T3, T4, T5
|
Zero-Halogen Lead-Free Ultra-Low-Temp Solder Paste 5RG |
Para sa mga espesyal na senaryo na pinahihintulutan lamang ang napakababang temperatura; |
0ppm ROL0 |
Uri ng Rosin |
In52Sn48/In40.2Sn20.7Bi39.1 haluang metal na pulbos T5, T6, T7 |
Water-Wash Lead-Free High-Temp Solder Paste 8MW1P/5RW1 |
Ang post-solder residue ay maaaring linisin ng tubig; mababang gastos; |
ORH1 |
Uri ng Water-Wash |
SC07/0307/105/305 haluang metal na pulbos T3, T4 |
Water-Wash Lead-Free Low-Temp Solder Paste 8MW1AP/5RW1A |
Hindi nag-iiwan ng mga bakas pagkatapos ng paghihinang sa nickel-plated aluminum heat sink fins; mababang gastos; |
ORH1 |
Uri ng Water-Wash |
Alloy powder tulad ng Sn42Bi58 T2.5, T3, T4 |
Laser Lead-Free High-Temp Solder Paste 5RLJ |
Laser-heated soldering na may superior performance at walang solder balls; tugma sa pneumatic, screw, at jet valve dispensing. |
<500ppm ROL0 |
Uri ng Rosin |
0307/105/305/00507BN/00507B2N haluang metal na pulbos T3, T4, T5, T6, T7 |
Laser Lead-Free Medium/Low-Temp Solder Paste 5RLJB |
Laser-heated soldering na may superior performance at walang solder balls; tugma sa pneumatic, screw, at jet valve dispensing. |
<500ppm ROL0 |
Uri ng Rosin |
Sn64Bi35Ag1/Sn64.7Bi35Ag0.3/Sn42Bi58/Sn42Bi57Ag1/Sn49.6Bi48.5Ag1Cu0.9/high-reliability LT32 at LT32S alloy powder T3, T4, T5, T6, T7
|
Lead-Free Solder Paste para sa Stainless Steel at Aluminum 8MW5/5RW5 |
Para sa paghihinang hindi kinakalawang na asero at aluminyo; maaaring linisin ng tubig |
ORH1 |
Uri ng Water-Wash |
SC07/0307/105/305/Sn64Bi35Ag1/Sn64.7Bi35Ag0.3/Sn42Bi58 haluang metal na pulbos T3, T4 |