| 姓名 | 參數 |
|---|---|
| 系列 | 零鹵無鉛超低溫錫膏5RG |
| 應用領域 | 只能承受超低溫的特殊場景 |
| 鹵素 | 0ppm ROL0 |
| 助焊劑類型 | 松香型 |
| 合金粉末 | In52Sn48/In40.2Sn20.7Bi39.1合金粉末,T5,T6,T7 |
匯集全系列錫膏、焊錫絲、焊條,提供適合各種SMT場景的焊接材料


| 姓名 | 參數 |
|---|---|
| 系列 | 零鹵無鉛超低溫錫膏5RG |
| 應用領域 | 只能承受超低溫的特殊場景 |
| 鹵素 | 0ppm ROL0 |
| 助焊劑類型 | 松香型 |
| 合金粉末 | In52Sn48/In40.2Sn20.7Bi39.1合金粉末,T5,T6,T7 |
LFP-JJY5RG-In52Sn48 zero-halogen ultra-low-temperature solder paste is made from In52Sn48 low-melting-point spherical alloy powder with zero-halogen control throughout. It uses a low-acid-value rosin-type ROL0 flux system, producing a fine, uniform paste with smooth printing of ultra-fine powder and stable low-temperature melting and wetting.
Adapted to special scenarios highly sensitive to thermal shock, such as heat-sensitive plastic components, PET flexible substrates, photosensitive chips, lithium battery protection boards and micro camera modules, its 118°C low melting point greatly shortens high-temperature exposure and avoids substrate blistering, internal component damage and flexible-board delamination or deformation. The mild-activity formula is gentle and does not corrode precision gold- or silver-plated micro pads, so ultra-thin circuits are safe from flux erosion.
The paste is a no-rosin-residue modified ROL0 rosin system that fully meets the IPC J-STD-004 zero-halogen standard. All raw materials and finished products pass authoritative SGS testing, with zero-halogen, REACH and RoHS all compliant. It leaves no irritating or corrosive residue, keeps the board bright and clean after soldering, and maintains high surface insulation resistance even without washing, ready for conformal coating or lamination downstream.
| Item | Specification | Reference Standard |
|---|---|---|
| Viscosity | 110±10Pa·S | IPC-TM-650 |
| Solder Ball | PASS | IPC-TM-650 |
| Printing Durability | Excellent | |
| Flux Content | 18±0.5% | |
| Flux Type | ROL0 | IPC J-STD-004 |
| Halogen Content | 0.0% | IPC J-STD-004 |
| Copper Mirror Corrosion Test | PASS | IPC-TM-650 |
| Surface Insulation Resistance - Initial | 1.0×1013Ω | IPC-TM-650 |
| Surface Insulation Resistance - After Humidity | 1.0×1012Ω | IPC-TM-650 |
| Spread Rate | 85% | JIS-Z-3197(1999) |
| Tack Life | 6-8 hours | |
| Solder Pit Test | Pass | IPC-TM-650 |
| Shelf Life (2-10°C) | 6 months | |
| Printability | Good printability with stencil apertures ≥65μm |
| Alloy | Main Components (%) | Impurity Content (%) | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| In | Sn | Pb | Sb | Fe | Zn | Cu | Bi | Al | As | Ni | Cd | |
| In52Sn48 | 52±0.5 | REM | <0.07 | <0.5 | <0.02 | <0.003 | <0.08 | <0.1 | <0.005 | <0.03 | <0.01 | <0.002 |
穩定的印刷黏度和初黏力,具有出色的成型性和高達 100% 的焊錫爬升高度。光亮,飽滿的焊點有效解決了冷焊點,焊橋,焊球,墓碑和空洞等行業難題。
通過多項環保 SGS 標準認證,包括 RoHS,鹵素和 REACH (SVHC)。焊接後殘留物透明無色,ROL0免清洗,絕緣電阻高,性能安全可靠。
來自德國和日本的先進生產和檢測設備,嚴格的ISO9001/ISO14001品質控制,每批21道檢驗步驟確保性能長期一致、穩定。
我們經驗豐富的工程師提供一對一服務,免費現場調試,以及更匹配的錫膏產品,現場解決焊接工藝問題。
全系列焊膏產品,滿足多樣化製程需求

SAC305合金,應用範圍廣,焊接可靠性高——當今應用最廣泛的環保焊膏

Sn42Bi58合金,熔點138℃,有效保護FPC等熱敏元件

Sn63Pb37共晶合金具有優異的焊接性能和成本效率,非常適合一般消費性電子產品
| 模型 | 應用 | 鹵素 | 類型 | 合金粉末 |
|---|---|---|---|---|
| 含鉛焊錫膏 8MN/7RN |
高活性,適合QFN/DFN高攀爬場景;焊點亮光亮; | 600~750ppm ROL1 |
松香型 | 62362/62836804/6337/6040等合金粉末 T2.5, T3, T4 |
| 含鉛焊錫膏 7M/7R |
適用於通訊,平板,筆記本,手機等高精準度,標準場景;焊點亮光亮; | 250~400ppm ROL0 |
松香型 | 62362/62836804/6337/6040/5545等合金粉末 T2.5, T3, T4, T5 |
| 含鉛焊錫膏 7MTWT/7RTWT |
適用於通訊、平板、筆記本、手機等高精度、標準場景;印刷後可承受長時間放置,且不會出現焊錫變黑或焊球;焊點亮光亮; | <500ppm ROL0 |
松香型 | 62362/62836804/6337/6040/5545/55X/50X/45X/40X/434314等合金粉末 T2.5, T3, T4, T5 |
| 含鉛焊錫膏 7MTHT/7RTHT |
致力於戶外顯示場景;穩定的黏度和較長的模板壽命(突出的優勢);焊接點光亮;濃縮松香殘留(無網版斑紋,墨色均勻) | 250~400ppm ROL0 |
松香型 | 62362/62836804/6337/6040等合金粉末 T2.5, T3, T4, T5 |
| 含鉛焊錫膏 7MH/7RH |
通用型,殘渣透明光亮;特別適用於LED等白板,耐乾燥性強,可連續列印16小時以上;焊膏可在室溫下保存;印刷後可承受長時間放置,不會出現焊料飛濺,尤其是無焊球 | 250~400ppm ROL0 |
松香型 | 62362/62836804/6337/6040/5545/55X/50X/45X/40X/434314等合金粉末 T2.5, T3, T4 |
| 含鉛焊錫膏 7ML/7RL |
殘渣透明光亮;特別適合LED等白板,耐乾燥性稍低,最適合快速消耗場景;也可用於凹槽嵌入式散熱器,以實現低空隙率 | 250~400ppm ROL0 |
松香型 | 62362/62836804/6337/6040/5545/55X/50X/45X/40X/434314等合金粉末 T2.5, T3, T4 |
| 含鉛焊錫膏 7MF/7RF |
鍍銀電子陶瓷元件、光伏電池、燈光玻璃屏等銀焊盤專用;不會腐蝕銀墊或導致變黑; | 150~350ppm ROL0 |
松香型 | 62362/62836804/6337/6040/5545等合金粉末 T2.5, T3, T4 |
| 水洗式含鉛焊錫膏 3MW9/3RW9 |
可水洗,成本較低,印刷成型性優異;也適用於儲能電池鉛柵焊接; | ORH1 | 水洗型 | 62362/62836804/6337/6040/5545/5050/4555/4060/3565/3070/2575/2080/1585/1090/595等合金粉末 T2.5, T3, T4 |
| 適用於不銹鋼和鋁的含鉛焊膏 3MW5/3RW5 |
用於焊接不銹鋼和鋁;可用水清洗 | ORH1 | 水洗型 | 62362/62836804/6337/6040/5545/5050/4555/4060/3565/3070/2575/2080/1585/1090/595等合金粉末 T2.5, T3, T4 |
| 含鉛合金類型 | 熔點(°C) | 焊接溫度(°C) | T2.5 | T3 | T4 | T4.5 | T5 | T6 | T7 |
|---|---|---|---|---|---|---|---|---|---|
| Sn62Pb36Ag2 | 179 | 200-225 | ✔ | ✔ | ✔ | ✔ | ✔ | ||
| Sn62.8Pb36.8Ag0.4 | 181 | 200-225 | ✔ | ✔ | ✔ | ✔ | ✔ | ||
| Sn63Pb36.9Ag0.1 | 181 | 200-225 | ✔ | ✔ | |||||
| 6337 (Sn63Pb37) | 183 | 200-225 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ |
| 6040 (Sn60Pb40) | 183-191 | 210-235 | ✔ | ✔ | ✔ | ||||
| 5545 (Sn55Pb45) | 183-203 | 225-245 | ✔ | ✔ | ✔ | ||||
| 5050 (Sn50Pb50) | 183-215 | 235-255 | ✔ | ✔ | ✔ | ||||
| 4555 (Sn45Pb55) | 183-227 | 245-265 | ✔ | ✔ | ✔ | ||||
| 4060 (Sn40Pb60) | 183-238 | 255-280 | ✔ | ✔ | ✔ | ||||
| 3565 (Sn35Pb65) | 183-248 | 265-290 | ✔ | ✔ | ✔ | ||||
| 3070 (Sn30Pb70) | 183-258 | 280-300 | ✔ | ✔ | ✔ | ||||
| 2575 (Sn25Pb75) | 183-260 | 280-300 | ✔ | ✔ | ✔ | ||||
| 2080 (Sn20Pb80) | 183-279 | 300-320 | ✔ | ✔ | ✔ | ||||
| 1585(Sn15Pb85) | 約。 183-285/295 | 305-335 | ✔ | ✔ | ✔ | ||||
| 1090(Sn10Pb90) | 268-301 | 320-340 | ✔ | ✔ | ✔ | ||||
| 595(Sn5Pb95) | 300-314 | 335-355 | ✔ | ✔ | ✔ | ||||
| Sn55/Pb41.5/Bi3/Sb0.5 | - | - | ✔ | ||||||
| Sn52/Pb42.5/Bi5/Sb0.5 | 170 | 190-220 | ✔ | ||||||
| Sn48/Pb48.6/Bi3/Sb0.4 | - | - | ✔ | ||||||
| Sn43/Pb49/Bi7/Sb1 | - | - | ✔ | ||||||
| Sn38/Pb52.5/Bi8/Sb1.5 | 173 | 190-220 | ✔ | ||||||
| Sn43Pb43Bi14 | 144-163 | 185-200 | ✔ | ✔ | ✔ | ||||
| Sn10Pb88Ag2 | 268-299 | 320-340 | ✔ | ✔ | |||||
| Sn5Pb92.5Ag2.5 | 287-296 | 315-335 | ✔ | ✔ | |||||
| Sn5Pb93.5Ag1.5 | 296-301 | 320-340 | ✔ | ✔ |
| 模型 | 應用 | 鹵素 | 類型 | 合金粉末 |
|---|---|---|---|---|
| 無滷無鉛高溫焊膏 8MQP/5RQ |
QFN/DFN 和類似應用具有高活性、最高焊錫爬升(接近 100%) | 單路 <900ppm / 雙路 <1500ppm ROL1 |
松香型 | 0307/105/305等合金粉末 T3, T4, T5 |
| 無滷無鉛高溫焊膏 8MTSP/5RTS |
更高的活性,良好的爬焊性(70%-90%),適用於 QFN/DFN 和類似應用;殘留物低,光亮; | <500ppm ROL0 |
松香型 | 0307/105/305等合金粉末 T3, T4, T5 |
| 無滷無鉛高溫焊膏 8MNTTP/5RNTT |
特別適合通訊,平板電腦,筆記型電腦,手機,藍牙,指紋鎖等高精度應用;殘留物低且透明; | 100~200ppm ROL0 |
松香型 | 0307/105/305/00507BN/00507B2N等合金粉末 T3, T4, T5 |
| 零鹵素和 REACH 無鉛高溫 8M9P/5RR |
零鹵素,極低空隙率,適用於汽車照明等低空隙,高導熱應用;殘留物低且透明; | 0ppm ROL0 |
松香型 | 0307/105/305等合金粉末 T3, T4, T5 |
| 無滷無鉛高溫焊膏 8MA |
適用於照明LED等通用、更寬間距的標準場景;殘留物低且透明; | <900ppm ROL1 |
松香型 | 0307/0107/SC07/00507BN/00507B2N合金粉末 T3, T4 |
| 標準無滷無鉛中低溫焊膏 8M/2R (8MTHL/2RTHL) |
適用於僅耐中低溫的無鉛中低溫場景,如LED,晶振,銅線燈,透明螢幕等; | 800~900ppm ROL1 |
松香型 | Sn64Bi35Ag1/Sn64.7Bi35Ag0.3/Sn42Bi58/Sn42Bi57Ag1/Sn49.6Bi48.5Ag1Cu0.9/高可靠性LT32S合金粉末 T2.5, T3, T4, T5 |
| 零鹵無鉛超低溫焊膏 5RG |
針對只能承受超低溫的特殊場景; | 0ppm ROL0 |
松香型 | In52Sn48/In40.2Sn20.7Bi39.1合金粉末 T5, T6, T7 |
| 水洗無鉛高溫焊膏 8MW1P/5RW1 |
焊接後殘留物可用水清洗;低成本; | ORH1 | 水洗型 | SC07/0307/105/305合金粉末 T3, T4 |
| 水洗無鉛低溫焊膏 8MW1AP/5RW1A |
焊接在鍍鎳鋁製散熱片上後不留痕跡;低成本; | ORH1 | 水洗型 | Sn42Bi58等合金粉末 T2.5, T3, T4 |
| 雷射無鉛高溫焊膏 5RLJ |
雷射加熱焊接,性能優越,無錫球;與氣動、螺桿和噴射閥點膠相容。 | <500ppm ROL0 |
松香型 | 0307/105/305/00507BN/00507B2N合金粉末 T3, T4, T5, T6, T7 |
| 雷射無鉛中低溫焊膏 5RLJB |
雷射加熱焊接,性能優越,無錫球;與氣動、螺桿和噴射閥點膠相容。 | <500ppm ROL0 |
松香型 | Sn64Bi35Ag1/Sn64.7Bi35Ag0.3/Sn42Bi58/Sn42Bi57Ag1/Sn49.6Bi48.5Ag1Cu0.9/高可靠性LT32和LT32S合金粉末 T3, T4, T5, T6, T7 |
| 適用於不銹鋼和鋁的無鉛焊膏 8MW5/5RW5 |
用於焊接不銹鋼和鋁;可用水清洗 | ORH1 | 水洗型 | SC07/0307/105/305/Sn64Bi35Ag1/Sn64.7Bi35Ag0.3/Sn42Bi58合金粉末 T3, T4 |
| 無鉛焊錫膏合金型 | 熔點(°C) | 焊接溫度(°C) | T2.5 | T3 | T4 | T4.5 | T5 | T6 | T7 |
|---|---|---|---|---|---|---|---|---|---|
| Sn96Ag4 | 221-226 | 240-260 | ✔ | ✔ | ✔ | ||||
| Sn97Ag3 | 221-224 | 240-260 | ✔ | ✔ | ✔ | ||||
| 305(Sn96.5Ag3Cu0.5) | 217 | 235-255 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | |
| 105(Sn98.5Ag1Cu0.5) | 221-227 | 240-260 | ✔ | ✔ | |||||
| 0307(Sn99Ag0.3Cu0.7) | 221-227 | 240-260 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | |
| 0107(Sn99.2Ag0.1Cu0.7) | 221-227 | 240-260 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | |
| 00507BN(SnCu0.7Ag0.05BiNi) | 221-227 | 240-260 | ✔ | ✔ | |||||
| 00507B2N(SnCu0.7Ag0.05Bi2Ni) | 221-227 | 240-260 | ✔ | ✔ | |||||
| 99307(Sn99.3Cu0.7) | 221-227 | 240-260 | ✔ | ✔ | |||||
| SC07NG(Sn99.3Cu0.7 (Ni0.04-0.07, Ge0.008-0.01)) | 227 | 240-260 | ✔ | ✔ | |||||
| Sn90Sb10 | 253.3-255.7 | 275-290 | ✔ | ✔ | ✔ | ✔ | |||
| Sn95Sb5 | 245 | 265-285 | ✔ | ✔ | ✔ | ✔ | |||
| Sn69.5Bi30Cu0.5 | 149-186 | 205-225 | ✔ | ✔ | |||||
| 64351(Sn64Bi35Ag1) | 151-172 | 195-220 | ✔ | ✔ | ✔ | ✔ | ✔ | ||
| 6473503(Sn64.7Bi35Ag0.3) | 151-172 | 195-220 | ✔ | ✔ | |||||
| 4258(Sn42Bi58) | 138 | 160-185 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | |
| Sn42Bi57Ag1 | 139/140 | 160-185 | ✔ | ✔ | ✔ | ✔ | ✔ | ||
| 高可靠性無鉛低溫 LT32/LT32S | 143-144 | 160-190 | ✔ | ✔ | ✔ | ✔ | ✔ | ✔ | |
| In52Sn48 | 118 | 140-160 | ✔ | ✔ | ✔ | ||||
| In40.2Sn20.7Bi39.1 | 65-89 | 110-130 | ✔ | ✔ | ✔ |
18年工藝-每一個細節都是品質的承諾
憑藉18年的研發和生產經驗以及科學開發的現代工藝配方,我們的焊膏與被焊接的零件高度相容,產生堅固、明亮、均勻、飽滿的焊點,無錫球。
開發出ROL0免清洗環保助焊劑,焊接後殘留物少,絕緣電阻高,保持板面清潔、無腐蝕,並形成保護層,防止基材再次氧化。
添加微量元素合金的優化助焊劑配方,結合特殊工藝,賦予焊膏高活性,充分潤濕焊盤,實現較高的爬焊高度,有效消除焊接過程中的冷焊,假焊,移位,立碑,錫球,空洞等問題。
焊錫粉顆粒圓整,大小均勻,印刷時無拉絲,沾黏,飛濺現象,成型後無塌陷,沾黏,起峰。連續印刷時黏度變化很小,漿料不會乾燥,黏性保持良好,不會造成材料損失。
焊接後殘留物會溶解並用純水(去離子水)洗掉,不留任何殘留物。清潔度非常高,在不損壞電子元件的情況下實現優異的ICT測試性能。生產及清潔過程無污染,符合環保要求。清潔速度很快——比其他類型的焊膏快得多。
遵循指南以獲得最佳性能
0-10℃冷藏;保存期限6個月
使用前2-4小時取出,達到室溫
徹底攪拌1-3分鐘至均勻
單獨密封並冷藏任何未使用的焊膏
多項權威認證,品質值得信賴
品質管理體系
符合 RoHS 標準
歐盟環保認證
18年工廠品牌

行業年資
顧客
檢查步驟
品質認證

我們的專業技術團隊根據您的工藝要求提供定製配方。焊料合金、助焊劑活性等級、清潔方法和特殊性能特徵均可客製化。我們還提供產品選擇建議、優化焊接流程並提供合適的解決方案來提高您的一次合格率。

5000平方公尺的工廠,配備96台生產和檢測設備。 ISO9001/ISO14001認證並嚴格執行。 21道檢測步驟確保焊接性能穩定。進料、過程中和成品測試可確保合規性。所有環保產品均經過 SGS 測試,符合 RoHS、無鹵素和 REACH (SVHC) 標準。

18年專注錫膏研發與生產。採用高純度原生錫,優化的助焊劑配方,添加微量元素合金的特殊製程。我們的焊膏精確匹配組裝場景,提供快速爬升和明亮,完整的焊點。無冷接頭,橋接,焊球,墓碑,空隙,拉絲,塌陷或乾燥問題。廠商直銷,無中間商,性價比更高。

資深工程師提供售前諮詢和售後技術支持,一對一服務。免費現場調試及產品匹配。現場解決問題。 24小時內提供解決方案,72小時內解決問題。品質問題免費更換。
服務多家知名企業,深受客戶信賴








免費樣品+技術工程師現場調試
微信支持

掃描添加我們微信