How to choose a suitable solder paste in SMT assembly?

Headlines
inSMTIn surface mount processing, solder paste is widely used inPCBAAssemblyPCBAManufacturing and all kinds ofSMTIn the process, forPCBAThe quality of the finished product plays a decisive role. Solder paste is a kind of soldering material,…
Why don't the solder joints shine after solder paste soldering?

Why don't the solder joints shine after solder paste soldering?

In solder paste surface mount processing and soldering, whether the solder joints are bright is also…
How to choose solder paste for SMT mounting?

How to choose solder paste for SMT mounting?

inSMTIn surface mount technology (SMT), different soldering processes often occur, so we need to cho…
Quality inspection of solder joints in SMT assembly

Quality inspection of solder joints in SMT assembly

In today's electronic product market, the development of various common electronic devices in life t…
【 JJY 】 Reasons and Solutions for Setting Up Monuments with Solder Paste

【 JJY 】 Reasons and Solutions for Setting Up Monuments with Solder Paste

With the emergence and development of microelectronic products, the requirements for circuit boards …
The causes of solder beads in SMT patch processing!

The causes of solder beads in SMT patch processing!

SometimesSMTTin beads will be produced during processing, which is a sign of poor processing. Genera…

contact

  • Tel:+86 0755 88366766
  • Phone:+86 18938660310
  • Email:sales@jjyhanxi.com
  • Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
  • Guangdong Public Security Backup 44030902002666 name
  • JJY TIN SOLDERWeChat
  • JJY TIN SOLDERWeChat official account
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.@All rights reserved. Low temperature tin wire, lead-free solder paste, lead solder paste