Brand:JIAJINYUAN/JJY
Model:LFP-JJY5RW-305T4
Alloy composition:Sn96.5Ag3.0Cu0.5
Particle size:4#(20-38um)
Viscosity:160±20Pa.S
Activity:Weak activity
Melting point:217℃
Working temperature:240-255(℃)
Specification:500g/bottle
+86 0755 88366766
LFP-JJY5RW-305T4Water-soluble water-washable lead-free high-temperature solder paste is adoptedSn96.5Ag3.0Cu0.5It is made of spherical solder powder of lead-free tin alloy with low oxidation degree and has excellent environmental protection characteristics,At the same time, it is a water-soluble water-washing paste refined from imported chemical materials, which is suitable for the soldering production process of electronic components with high cleanliness requirements. The coffee-colored residue after welding can be dissolved and washed off with pure water (deionized water), but it does not change after cleaningLeaving any residue can achieve excellent resultsICTTest the performance without causing damage to electronic components. The production and cleaning processes do not cause pollution and meet environmental protection requirements. It has a fast cleaning speed, much faster than other types of solder paste. It has good demolding performance during printing, excellent dry resistance and good thixotropic performance, and can be applied to general spacings≧0.3mmThe printing of pads and the mounting of most components. When printing continuously, the viscosity change is small, which can ensure the stability of the printing effect during long-term operation. This product has excellent thixotropic performance and maintains a good shape after printing,It is not easy to collapse and avoids the displacement of surface mount components. The weld points are bright after welding and have excellent electrical conductivity. Fewer solder beads are produced during welding, reducing the occurrence of short circuits.
The on-time delivery rate is as high as99%
It is suitable for electronic components with high cleanliness requirementsSMTThe production process of surface mount soldering. The coffee-colored residue after welding can be dissolved and washed off with pure water (deionized water). After cleaning, no residue is left, which can achieve an excellent effectICTTest the performance without causing damage to electronic components. The production and cleaning processes do not cause pollution and meet environmental protection requirements. It has a fast cleaning speed, much faster than other types of solder paste.
Technical parameters
Technical Parameters
in2-10℃The storage period under the environment is6Months, not less than0℃Store under such conditions and thaw before use2-4It should be left to room temperature for more than an hour before opening to prevent the formation of tin beads due to moisture. Then stir well before use.
Our experts tailor solder alloys, flux activity levels, cleaning methods, and specialty properties to your process. We optimize welding parameters and recommend application-specific solutions, boosting your first-pass yield.
5,000㎡ facility with ISO9001-certified and production & testing equipments. Full-process inspection: raw materials, processes, and finished products. SGS-certified eco-compliance: ROHS, REACH, ELV.
High-purity tin with lower dross rate than industry average. Fast wetting | Robust & glossy joints | Zero defects (cold joints, bridging, collapse,etc.). Factory-direct pricing for maximum cost efficiency.
Provide technical support: 24-hour response | 72-hour full resolution. Free material replacement & solder dross recycling. Pre-sales consultation & post-sales troubleshooting.
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.Founded in October 2008, is a collection of electronic solder R & D, production, customization, solutions, services in one of the customized solder solutions provider, “JIAJINYUAN” has been selected as a strong brand national demonstration project [solder materials]. Jiajinyuan factory covers an area of more than 5,000 square meters, with a number of modern production equipment, testing equipment and laboratory equipment. Our lead-free solder products have passed the “SGS” test and are fully compliant with the latest EU RoHS directive and REACH standard ....... If you have any questions, please feel free to contact us!
Service Hotline:+86 075588366766
Phone: +86 18938660310
Fax: +86 0755 88367866
QQ: 2790138382
Email: sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
National Service Hotline
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account