Soldering Technology, Tin Leads The FutureOne Stop Electronic Tin Soldering Solution Supplier

Tin-Lead Solder Wire
Leaded solder wire Sn45

Brand:JIAJINYUAN/JJY

Alloy composition:Sn45

Customized processing: Yes

Welding wire diameter:1.0(mm)

Melting point:183-230(℃)

Whether it conforms or notRoHSYes (fits)

Weldable: Copper parts, tin-plated copper parts, etc

Working temperature:  230~270(℃)

Specification:800(g)

Product Description product description
Leaded solder wireSn45<="" iv="">

Leaded solder wireSn45It is to fuse and electrolyze lead using high-purity tin raw materials from tin ore,It is refined through a special process; The rosin core of the product is made by boiling high-quality pure white transparent hydrogenated rosin in a vacuum sealed container with self-developed organic acid active agents. The process is special and reliable.

On-time deliveryThe on-time delivery rate is as high as99%
Scope of application Scope of application
Wide range It is suitable for soldering on circuit boards, with fast tin application, bright and full solder joints, few tin explosions, good fluidity and high mechanical strength.
Product display Product Show

Leaded solder wire without cleaning<="">

Leaded solder wire without cleaning<="">

Product Features Product characteristic
  • 1 Stable performance and safe to use Precise process control ensures that the rosin flux is evenly and continuously distributed, with no interruption of rosin. The soldering speed is fast, without sharpening or splashing. Customized tin wires with high compatibility can be made according to requirements.
  • 2The weld points are bright and the workmanship is excellent Strictly adhering to national standards, it is made of high-purity virgin refined tin, electrolytic copper and pure silver materials, with few elemental impurities, sufficient degree, bright surface of the tin wire, uniform winding without tangling, little smoke and no unpleasant smell during welding, bright and firm weld points, and strong reliability.
  • 3 It has good wettability and is easy to tin The self-developed flux can remove the oxide layer and surface oil stains of the soldered material, reduce the surface tension of the soldered material, increase the welding area, has good wettability, is easy to tin, and has no bridging.
  • 4 Luoyang Iron has less scum and requires no cleaning Adopting a scientific rosin flux formula, it is strictly produced in accordance with national and EU standards, ensuring excellent solderability while guaranteeing low corrosiveness of the flux, fast welding speed and minimal residue after welding.