Dispensing syringe solder paste, as a basic consumable in the field of electronic soldering, is widely used in both fully automatic and manual dispensing machines as a dispensing consumable. Introduction to the application of dispensing syringe type solder paste by solder paste manufacturers:
Solder paste is mainly composed of solder powder, flux paste, its surfactant and thixotropic agent. The key to solder paste lies in its wide application inLEDSemiconductor materials, photovoltaic products, surveillance cameras, electrical connection wires, etc., the key lies in the combination of welding processes, conductivity and other effects.
The wide application of solder paste mainly lies in where it is usedSMT,PCBThe soldering process of the board and the tinning of the pins of electronic components are carried out to ensure high reliability and obvious effects of the soldering process. It is applicable to the soldering process of various surface mount electronic devices.
In the professional field of solder paste, bubbles should be avoided in the solder paste of the syringe. In the professional packaging technology of JJY, the packaging process of improving the mixing vacuum has avoided the formation of bubbles as much as possible. If there are bubbles in the solder paste of the syringe, the solder will break halfway, and bubbles will appear at the dispensing port. This may lead to frequent solder breakage, bubbles, and incomplete dispensing throughout the dispensing process.
Shenzhen JJYDispensing syringe type solder pasteThe manufacturer has carried out mutually beneficial cooperation with electronic solder user manufacturers. With a rich variety of successful product research and development cases, the overall strength has created a high-quality and trustworthy sales market.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account