Reflow soldering technology is heresmtThe field of surface mount technology (SMT) processing is no stranger. The components on various boards used in our computers are all soldered onto the circuit board through this process. There is a heating circuit inside that heats air or nitrogen to a sufficiently high temperature and then blows it onto the already attached circuit board, causing the solder on both sides of the component to melt and bond with the main board. The following is JJYSolder paste manufacturerI will take you to have a look:
The main factors affecting the glossiness of reflow solder joints
1The composition of solder paste is different, which will affect the gloss of the solder joints. For example, the solder joints presented are different when the solder paste contains silver and when it does not.
2Whether the tin powder in the solder paste is oxidized or not will cause differences in the gloss of the solder joints.
3Whether there are any additives in the flux itself in the solder paste that form a matting effect;
4During the reflow soldering process, if the reflow soldering temperature is insufficient or too high, causing the flux to evaporate prematurely, it will directly affect the gloss of the solder joint.
5In reflow soldering, the preheating temperature of reflow soldering is relatively low, and there may be substances that are difficult to evaporate remaining on the surface of the solder pad, which will affect the gloss of the reflow solder joint
6After reflow soldering, whether there is rosin or other impurities remaining on the surface of the solder joint is a common phenomenon, which will affect the gloss of the solder joint.
15For many years, JJY has been dedicated to the research and development, production and sales of solder paste, solder wire and solder bar, providing customers with a complete set of electronic soldering solutions. If you want to learn more about solder paste, please keep following JJY Solder Paste Manufacturer and leave a message online to interact with us.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account