Brand:JIAJINYUAN/JJY
Alloy composition:Sn99.3Cu0.7
Customized processingis
Welding wire diameter: 0.8(mm)
Melting point:227(℃)
Whether it conforms or notRoHS:Yes (conforms to)
Weldable: Copper parts, tin-plated copper parts, etc
Working temperature:280~300(℃)
Specification:50~20000(g)
+86 0755 88366766
Halogen-free, environmentally friendly and lead-free solder wire is made by dissolving and refining lead-free pure tin, pure copper and pure silver in proportion with other environmentally friendly alloys at high temperatures, removing impurities and casting them into tin cylinders. Then, it is pressed and cast with a hydraulic press and flux (rosin agent). Solder wires of different sizes are produced and drawn by a wire drawing machine according to different wire diameter requirements. The alloy composition is divided into tin-copper, tin-silver, tin-silver-copper alloy or other alloys. The flux is evenly poured into the middle part of the tin alloy.
The on-time delivery rate is as high as99%
Used for compliance with all requirementsRoHSThe welding of environmentally friendly electronic components and other workpieces as instructed.
Our experts tailor solder alloys, flux activity levels, cleaning methods, and specialty properties to your process. We optimize welding parameters and recommend application-specific solutions, boosting your first-pass yield.
5,000㎡ facility with ISO9001-certified and production & testing equipments. Full-process inspection: raw materials, processes, and finished products. SGS-certified eco-compliance: ROHS, REACH, ELV.
High-purity tin with lower dross rate than industry average. Fast wetting | Robust & glossy joints | Zero defects (cold joints, bridging, collapse,etc.). Factory-direct pricing for maximum cost efficiency.
Provide technical support: 24-hour response | 72-hour full resolution. Free material replacement & solder dross recycling. Pre-sales consultation & post-sales troubleshooting.
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.Founded in October 2008, is a collection of electronic solder R & D, production, customization, solutions, services in one of the customized solder solutions provider, “JIAJINYUAN” has been selected as a strong brand national demonstration project [solder materials]. Jiajinyuan factory covers an area of more than 5,000 square meters, with a number of modern production equipment, testing equipment and laboratory equipment. Our lead-free solder products have passed the “SGS” test and are fully compliant with the latest EU RoHS directive and REACH standard ....... If you have any questions, please feel free to contact us!
Service Hotline:+86 075588366766
Phone: +86 18938660310
Fax: +86 0755 88367866
QQ: 2790138382
Email: sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
National Service Hotline
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account