  • Silver-free lead-free solder wire
  • Silver-free lead-free solder wire

Silver-free lead-free solder wire

Brand:JIAJINYUAN/JJY

Alloy composition:Su99.3cu0.7

Processing and customization: Yes

Welding wire diameter: 0.8(mm)

Melting point:227(℃)

Whether it conforms or notRoHSYes (fits)

Weldable: Copper parts, tin-plated copper parts, etc

Working temperature:280~300(℃)

Specification:50~20000(g)

Order Hotline

+86 0755 88366766

Product Description PRODUCT DESCRIPTION

Silver-free lead-free solder wire

Silver-free lead-free solder wire is made by adding lead-free pure tin, pure copper, pure silver in proportion to other environmentally friendly alloys, dissolving them at high temperatures, refining, removing impurities, and casting them into tin cylinders. Then, it is pressed and cast with a hydraulic press and flux (rosin agent). Solder wires of different sizes are produced and drawn by a wire drawing machine according to different wire diameter requirements. The alloy composition is divided into tin-copper, tin-silver, tin-silver-copper alloy or other alloys. The flux is evenly poured into the middle part of the tin alloy.

On-time deliveryThe on-time delivery rate is as high as99%
Scope of application SCOPE OF APPLICATION
Wide range Used for compliance with all requirementsRoHSThe welding of environmentally friendly electronic components and other workpieces as instructed.
Product display PRODUCT SHOW

Silver-free lead-free solder wire

Silver-free lead-free solder wire

Product Features PRODUCT CHARACTERISTIC
  • 1 Stable performance and safe to use Precise process control ensures that the rosin flux is evenly and continuously distributed, with no interruption of rosin. The soldering speed is fast, without sharpening or splashing. Customized tin wires with high compatibility can be made according to requirements.
  • 2The weld points are bright and the workmanship is excellent Strictly adhering to national standards, it is made of high-purity virgin refined tin, electrolytic copper and pure silver materials, with few elemental impurities, sufficient degree, bright surface of the tin wire, uniform winding without tangling, little smoke and no unpleasant smell during welding, bright and firm weld points, and strong reliability.
  • 3 It has good wettability and is easy to tin The self-developed flux can remove the oxide layer and surface oil stains of the soldered material, reduce the surface tension of the soldered material, increase the welding area, has good wettability, is easy to tin, and has no bridging.
  • 4 Luoyang Iron has less scum and requires no cleaning Adopting a scientific rosin flux formula, it is strictly produced in accordance with national and EU standards, ensuring excellent solderability while guaranteeing low corrosiveness of the flux, fast welding speed and minimal residue after welding.
Company Advantages
JJY

Advanced R&D Team Custom Solutions for Clients

Our experts tailor solder alloys, flux activity levels, cleaning methods, and specialty properties to your process. We optimize welding parameters and recommend application-specific solutions, boosting your first-pass yield.

JJY

Rigorous Quality Control Consistent Performance Stability

5,000㎡ facility with ISO9001-certified and production & testing equipments. Full-process inspection: raw materials, processes, and finished products. SGS-certified eco-compliance: ROHS, REACH, ELV.

JJY

17 Years Experience Superior Welding Results

High-purity tin with lower dross rate than industry average. Fast wetting | Robust & glossy joints | Zero defects (cold joints, bridging, collapse,etc.). Factory-direct pricing for maximum cost efficiency.

JJY

24/7 Technical Support Onsite Engineers Services

Provide technical support: 24-hour response | 72-hour full resolution. Free material replacement & solder dross recycling. Pre-sales consultation & post-sales troubleshooting.

Company Profiles
JJY

SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.Founded in October 2008, is a collection of electronic solder R & D, production, customization, solutions, services in one of the customized solder solutions provider, “JIAJINYUAN” has been selected as a strong brand national demonstration project [solder materials]. Jiajinyuan factory covers an area of more than 5,000 square meters, with a number of modern production equipment, testing equipment and laboratory equipment. Our lead-free solder products have passed the “SGS” test and are fully compliant with the latest EU RoHS directive and REACH standard ....... If you have any questions, please feel free to contact us!

Contact Us

JJY

SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.
  • Service HotlineService Hotline:+86 075588366766

Phone: +86 18938660310

Fax: +86 0755 88367866

QQ: 2790138382

Email: sales@jjyhanxi.com

Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)

MESSAGE

Recommended hot products / Hot product

Common solder wire Sn99.3Cu0.7

Common solder wire Sn99.3Cu0.7

Brand:JIAJINYUAN/JJY Alloy composition:Su99.3cu0.7 Processing and customization: Yes Welding wire diameter:0.8(mm) Melting point:227(℃) Whether it conforms or notRoHSYes (fits) Weldable:Copper parts, tin-plated copper parts, etc Working temperature:280~300(℃) Specification:50~20000(g)
Lead-free tin wire Sn99.3Cu0.7

Lead-free tin wire Sn99.3Cu0.7

Brand:JIAJINYUAN/JJY Alloy composition:Su99.3cu0.7 Processing and customization: Yes Welding wire diameter:0.8(mm) Melting point:227(℃) Whether it conforms or notRoHSYes (fits) Weldable:Copper parts, tin-plated copper parts, etc Working temperature:280~300(℃) Specification:50~20000(g)
Lead-free solder wire containing silver 3.0

Lead-free solder wire containing silver 3.0

Brand:JIAJINYUAN/JJY Alloy composition:Su96.5Ag3.0cu0.5 Processing and customization: Yes Welding wire diameter:0.8(mm) Melting point:227(℃) Whether it conforms or notRoHSYes (fits) Weldable:Copper parts, tin-plated copper parts, etc Working temperature:280~300(℃) Specification:50~20000(g)
Silver-free lead-free solder wire

Silver-free lead-free solder wire

Brand:JIAJINYUAN/JJY Alloy composition:Su99.3cu0.7 Processing and customization: Yes Welding wire diameter:0.8(mm) Melting point:227(℃) Whether it conforms or notRoHSYes (fits) Weldable:Copper parts, tin-plated copper parts, etc Working temperature:280~300(℃) Specification:50~20000(g)

National Service Hotline

+86 0755 88366766
+86 18938660310

contact

  • Tel:+86 0755 88366766
  • Phone:+86 18938660310
  • Email:sales@jjyhanxi.com
  • Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
  • Guangdong Public Security Backup 44030902002666 name
  • JJY TIN SOLDERWeChat
  • JJY TIN SOLDERWeChat official account
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.@All rights reserved. Low temperature tin wire, lead-free solder paste, lead solder paste