Brand:JIAJINYUAN/JJY
Model:LFP-H-4258
Alloy composition:Sn42Bi58Cu0.3
Particle size:20-38(um)
Viscosity:200(Pa·S)
Activity: Weak activity
Melting point:138℃
Working temperature:235-250(℃)
Specification:500g/bottle
+86 0755 88366766
Lead-free solder pasteLFP-H-4258It is developed by using special flux and spherical tin powder with very low oxide content, and adopts a conformingRosin Mildly Activated Classification of Federal specificationThe required non-halogen activation system This solder paste isRMAFlux and tin powder particles are uniformly mixed. The solder paste contained in this product complies with the standards of the United StatesQQ-571As stipulated in itRMAType and passSGSTest compliantRoHSInstruction requirements.
The on-time delivery rate is as high as99%
Only resistant to medium and low temperaturesLEDLead-free medium-temperature and lead-free low-temperature scenarios such as crystal oscillators, copper wire lamps and glass screens for light shows;
| Project | Parameters | |
| Appearance | The appearance is light gray, smooth and paste-like without layering | |
| Flux content(wt%) | 11±0.5 | |
| Halogen content(wt%) | RMAtype | |
| Viscosity(25℃whenpa.s) | 200(±10%) | |
| Particle volume(μm) | 25~45 | |
| The water jet takes impedance(Ω·cm) | >1×105 | |
| Silver tinate paper test | Qualified | |
| Copper plate corrosion test | Qualified | |
| Surface insulation impedance test(Ω) | 40℃/90%RH | >1×1013 |
| 80℃/85%RH | >1×1012 | |
| Expansion rate(%) | >90 | |
| Tin bead test | Qualified | |
|
Note: The test method is applicableJIS.Z.3282andANSI/J-STD-006
Composition of tin powder alloyJIS.Z.3910
The performance Pointers listed in this table are reference values, and the actual values are from each batch of deliveryQAThe report shall prevail.
|
||
in5-10℃The storage period under the environment is6Months, not less than0℃Store under such conditions and thaw before use2-4It should be left to room temperature for more than an hour before opening to prevent the formation of tin beads due to moisture. Then stir well before use.
Our experts tailor solder alloys, flux activity levels, cleaning methods, and specialty properties to your process. We optimize welding parameters and recommend application-specific solutions, boosting your first-pass yield.
5,000㎡ facility with ISO9001-certified and production & testing equipments. Full-process inspection: raw materials, processes, and finished products. SGS-certified eco-compliance: ROHS, REACH, ELV.
High-purity tin with lower dross rate than industry average. Fast wetting | Robust & glossy joints | Zero defects (cold joints, bridging, collapse,etc.). Factory-direct pricing for maximum cost efficiency.
Provide technical support: 24-hour response | 72-hour full resolution. Free material replacement & solder dross recycling. Pre-sales consultation & post-sales troubleshooting.
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.Founded in October 2008, is a collection of electronic solder R & D, production, customization, solutions, services in one of the customized solder solutions provider, “JIAJINYUAN” has been selected as a strong brand national demonstration project [solder materials]. Jiajinyuan factory covers an area of more than 5,000 square meters, with a number of modern production equipment, testing equipment and laboratory equipment. Our lead-free solder products have passed the “SGS” test and are fully compliant with the latest EU RoHS directive and REACH standard ....... If you have any questions, please feel free to contact us!
Service Hotline:+86 075588366766
Phone: +86 18938660310
Fax: +86 0755 88367866
QQ: 2790138382
Email: sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
National Service Hotline
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account