Soldering Technology, Tin Leads The FutureOne Stop Electronic Tin Soldering Solution Supplier

Lead-Free Solder Bar
Lead-free tin bar Sn99Ag0.3Cu0.7

Brand:JIAJINYUAN/JJY

Alloy composition:Sn99Ag0.3Cu0.7

Length: 326(mm)

Welding wire diameter: 0.8(mm)

Melting point:227(℃)

Whether it conforms or notRoHSYes (fits)

Weldable: Copper parts, tin-plated copper parts, etc

Working temperature:260~300(℃)

Specification:50~20000(g)

Product Description product description

Environmentally friendly lead-free tin bars<="">

Lead-free tin bars are made by fusing high-purity tin raw materials from tin ore into electrolytic copper. They are produced through a special manufacturing method and a high-standard production process, and are cast by dedicated engineers under precise instrument inspection and quality control. The product has strong oxidation resistance, excellent physical and chemical properties, does not pollute the environment, and meets national standardsJIS, IPCSuch standards.

On-time deliveryThe on-time delivery rate is as high as99%
Scope of application Scope of application
Wide range Used for compliance with all requirementsRoHSWave soldering or dip soldering of environmentally friendly electronic components and other workpieces as instructed.
Product display Product Show

Environmentally friendly lead-free tin bars<="">

Environmentally friendly lead-free tin bars<="">

Product Features Product characteristic
  • 1 The speed of going to tin is very fast Strictly adhering to national standards, it is made of high-purity primary refined tin, electrolytic copper and pure silver materials. After melting, it has low viscosity, good wettability, high fluidity, excellent solderability and is easy to solder, effectively improving the welding efficiency.
  • 2Strong antioxidant capacity The proprietary anti-oxidation alloy technology endows the tin bars with unique anti-oxidation properties, ensuring a very low oxidation slag production rate during the welding process and reducing unnecessary waste.
  • 3 The weld points are bright and firm After special process adjustment and refining treatment, the metallographic particles are very fine, the weld points are firm, bright and full, without false welding, voids, sharp points or bridging phenomena, and there are no residual impurities after welding.
  • 4 Ultra-low slag discharge technology The unique high-antioxidant formula, combined with free on-site technical services provided by engineers, such as reasonable setting of temperature, peak height, chain speed, slag removal and tin strip addition time points, inspection and correction of components, flux compatibility, etc. To effectively maintain the stability of solder composition, find the balance point between efficiency and stability, and control the slag discharge rate at7~20%. Free on-site tin cleaning service. High price for tin slag recycling or exchange for brand new tin bars.