Brand:JIAJINYUAN/JJY
Model:LFP-JJY8MHP-0307T5
Alloy composition:Sn99Ag0.3Cu0.7
Particle size:5#(15-25um)
Viscosity:190±20Pa.S
Activity: Weak activity
Melting point:216~227℃
Peak temperature:230-240(℃)
Specification:500g/bottle
<="">
The on-time delivery rate is as high as99%
Suitable for high activityQFN/DFNDedicated scene for climbing Xigao;| Project | Parameters | |
| Appearance | The appearance is light gray, smooth and paste-like without layering | |
| Flux content(wt%) |
11.8%±12%
|
|
| Halogen content(wt%) |
<0.05%
|
|
| Viscosity(25℃whenpa.s) |
190±20Pa.S
|
|
| Particle volume(μm) | 20~38 | |
| The water jet takes impedance(Ω·cm) | >1×105 | |
| Silver tinate paper test | Qualified | |
|
Copper mirror corrosion test
|
PASS | |
| Surface insulation impedance test(Ω) | Initial value |
1.0×10
13Ω
|
| After the hot and humid weather |
1.0×1012Ω
|
|
| Expansion rate(%) |
85%
|
|
| Tin bead test | PASS | |
| Note: The test method is applicableJIS.Z.3282andANSI/J-STD-006 |
||
<="">
in5-10℃The storage period under the environment is6Months, not less than0℃Store under such conditions and thaw before use2-4It should be left to room temperature for more than an hour before opening to prevent the formation of tin beads due to moisture. Then stir well before use.