Brand:JIAJINYUAN/JJY
Alloy composition:Sn99.3Cu0.7
Customized processingis
Welding wire diameter: 0.8(mm)
Melting point:227(℃)
Whether it conforms or notRoHS:Yes (conforms to)
Weldable: Copper parts, tin-plated copper parts, etc
Working temperature:280~300(℃)
Specification:50~20000(g)
Stainless steel environmental-friendly lead-free solder wire is made by dissolving, refining and removing impurities from lead-free pure tin, pure copper and pure silver in proportion with other environmental-friendly alloys at high temperature, casting them into tin cylinders, and then die-casting them with a hydraulic press and flux (rosin agent). It is produced and drawn into solder wires of different sizes according to different wire diameter requirements by a wire drawing machine. The alloy composition is divided into tin-copper, tin-silver, tin-silver-copper alloy or other alloys. The flux is evenly poured into the middle part of the tin alloy.
The on-time delivery rate is as high as99%
Used for compliance with all requirementsRoHSThe welding of environmentally friendly electronic components and other workpieces as instructed.