Brand:JIAJINYUAN/JJY
Alloy composition:Su99Ag0.3cu0.7
Processing and customization: Yes
Welding wire diameter: 0.8(mm)
Melting point:227(℃)
Whether it conforms or notRoHSYes (fits)
Weldable: Copper parts, tin-plated copper parts, etc
Working temperature:280~300(℃)
Specification:50~20000(g)
<="">
containing0.3Silver lead-free solder wire is made by mixing lead-free pure tin, pure copper, pure silver in proportion with other environmentally friendly alloys, dissolving them at high temperatures, refining them, removing impurities, casting them into tin cylinders, and then pressing them with a hydraulic press and flux (rosin agent). It is produced and drawn into solder wires of different sizes according to different wire diameter requirements using a wire drawing machine. The alloy composition is divided into tin-copper, tin-silver, tin-silver-copper alloy or other alloys. The flux is evenly poured into the middle part of the tin alloy.
The on-time delivery rate is as high as99%
Used for compliance with all requirementsRoHSThe welding of environmentally friendly electronic components and other workpieces as instructed.
<="">
<="">