Brand:JIAJINYUAN/JJY
Alloy composition:Sn42Bi58
Processing and customization: Yes
Welding wire diameter: 0.8(mm)
Melting point:138(℃)
Whether it conforms or notRoHSYes (fits)
Weldable: Copper parts, tin-plated copper parts, etc
Working temperature:190~200(℃)
Specification:50~20000(g)
<="">
Low-temperature environmentally friendly lead-free solder wire is made by dissolving, refining and removing impurities from lead-free pure tin, pure copper and pure silver in proportion with other environmentally friendly alloys at high temperatures, casting them into tin cylinders, and then die-casting them with a hydraulic press and flux (rosin agent). It is produced and drawn into solder wires of different sizes according to different wire diameter requirements by a wire drawing machine. The alloy composition is divided into tin-copper, tin-silver, tin-silver-copper alloy or other alloys. The flux is evenly poured into the middle part of the tin alloy.
The on-time delivery rate is as high as99%
Used for compliance with all requirementsRoHSThe welding of environmentally friendly electronic components and other workpieces as instructed.
<="">