Lead-free low-temperature solder pasteIt is one of the commonly used soldering materials in electronic manufacturing at present. Compared with lead-containing solder paste, its advantages are obvious. It is non-toxic, environmentally friendly and easy to reflux, and has become a development trend. When the surface mount component cannot withstand more than180℃When the temperature is high and a surface mount reflow process is required, we will use lead-free low-temperature solder paste for soldering. So, what is the melting point of lead-free low-temperature solder paste? Shenzhen solder paste manufacturers will explain it to everyone:
The main component of low-temperature lead-free solder paste isSn42Bi58The melting point is138℃It is the solder paste with the lowest melting point among lead-free solder pastes. Because it contains no lead and has a low melting point, it can prevent electronic components from being scorched by high temperatures during the soldering process, such as plastic and switch components, andLEDFor components like small light beads, lead-free low-temperature solder paste is quite suitable.
The particle size of the tin powder in lead-free low-temperature solder paste is between25~45or20~38umBetween them, the working temperature of reflow soldering is usually at170℃-180℃. It has strong weldability, good wettability, and very little residue after welding, especiallyledNowadays, many manufacturers in the industry prefer lead-free low-temperature solder paste as the soldering material.
It should be noted that in low-temperature lead-free solder pasteBiThe content has reached58%Therefore, it is slightly inferior to lead-containing solder paste in terms of soldering firmness. This situation can be selected based on the actual circumstances. If you want to know about lead-free solder paste, flux paste and leaded solder paste, please follow the online message of JJY Solder Paste Manufacturer to interact with us.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account