SMTDuring the production process of surface mount technology (SMT) processing, many different processing defect phenomena may occur. Different environments and operation methods can lead to different processing defects.SMTSurface mount technology (SMT) is also a precision processing method. It is normal for some problems to occur. What needs to be done is to control the quality during processing and solve all possible problems. Now, Shenzhen JJY Solder Paste Manufacturer will briefly introduce to you how to prevent the occurrence of solder paste defects:
Solder pastePrinting isPCBA crucial link in the assembly process. However, due to the complex influence of various factors such as printing equipment, materials and process parameters, solder paste printing often has defects, such as poor adhesion, solder pad spatter and poor solder joints. These issues may lead to a decline in product quality and a reduction in production efficiency, causing trouble for your business.
At JJY, we are committed to resolving solder paste printing defects to ensure the smooth progress of your production. We possess advanced R&D and production technologies and offer you the following solutions:
1Precise formula design: The solder paste of JJY has been carefully formulated to ensure excellent wettability and controllability during the printing process, thereby reducing adhesion issues.
2High-precision printing control: Our solder paste printing technology features high-precision printing control capabilities, including precise regulation of parameters such as printing pressure, speed, and squeegee Angle, to reduce solder pad spatter and the occurrence of poor solder joints.
3Optimize process parameters: The professional team of JJY will optimize the process parameters for solder paste printing based on your specific needs to ensure the best printing results and quality stability.
4Comprehensive technical support: Our technical team will provide you with comprehensive technical support, including process optimization, troubleshooting and training, etc., to ensure that you achieve the best results in the solder paste printing process.
JJY Solder Paste Factory produces a wide range of solder paste products, including lead-free solder paste, halogen-free solder paste, silver-containing lead solder paste, syringe solder paste, nickel-plated environmentally friendly solder wire, solder bar, etc. We can provide technical support. If you have any needs or technical questions regarding soldering, please feel free to leave a message online to interact with us!
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account