There is lead solder pasteIt is a kind of solder paste that does not require cleaning. The proportion of tin is approximately63%The lead content is approximately37%. Solder paste is used for soldering electronic connectors, terminals, circuit boards and other components to achieve conductive connections and has excellent continuous printing performance. Less residue and good electrical conductivity; In addition, no-wash solder paste can offer various alloy compositions, different tin particle sizes and different metal contents to meet customers' requirements for different products and processes. Next, JJY solder Paste Manufacturer will talk about the advantages and disadvantages for everyone:
I. Advantages of lead-based solder paste:
1It features high welding strength, good electrical conductivity and can maintain the welding effect for a long time.
2It has a wide range of applications and can be used for various different welding substrates and processes.
3The price is relatively low and it has a high cost performance.
2. Disadvantages of leaded solder paste:
1The surface oxidation rate is fast after welding, and antioxidants need to be used for protection.
2The color after welding differs significantly from that of the base material, which affects the appearance.
3It contains harmful substances such as lead, which have certain negative impacts on human health and the environment.
JJY Technology Co., Ltd. is a company engaged in the soldering industry16A manufacturer specializing in the research and development and customization of solder, solder paste, lead-free solder paste and leaded solder paste for many years. If you want to learn more about solder paste, please keep following the online message of JJY Solder Paste Manufacturer to interact with us.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account