Compared with tin alloys without silver, tin alloys with silver usually perform better during the tinning process, mainly because the addition of silver can improve certain properties of tin alloys. Then why is tin containing silver better for tin plating than that without silver? BelowTin wire manufacturerLet me explain:
The following are some reasons why silver-containing tin is better tinned than non-silver-containing tin:
1Silver can improve the wettability of tin alloy, making it easier to spread evenly on the welding surface, which is very important for ensuring the uniformity and quality of the welding.
2The addition of silver can enhance the fluidity of tin alloys, making them easier to coat and melt during the welding process. This is crucial for achieving precise soldering on the tiny solder joints of electronic components.
3The presence of silver can improve the mechanical properties of solder joints, including strength and durability, which is crucial for ensuring the reliability and longevity of welded connections.
4The addition of silver usually enables effective welding at lower temperatures, which is highly beneficial for applications where the welding materials are temperature-sensitive.
5Silver can reduce the oxidation tendency of tin alloys, which helps to slow down the oxides that may be produced during the welding process and improve the quality of the welding connection.
The above is what the editor of JJY has shared with you about why tin containing silver is better than tin without silver. In short, tin alloys containing silver perform better in terms of wettability, fluidity, strength, durability and oxidation resistance, which makes them more common in electronic manufacturing and other applications that require high-quality soldering. However, in some specific applications, there may be a demand for silver-free tin alloys, which usually depends on the specific requirements and application scenarios.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account