Recently, JJY received feedback from a customer of an electronics manufacturer:In useSolder pasteDuring the printing process, the problem of the solder paste turning black occurred. In response to this issue, we immediately organized capable personnel to conduct an analysis and discussion. First of all, the quality of the solder paste was reviewed. From raw materials to production and then to the packaging of the finished product, every step was carefully examined. It was found that the quality of the solder paste was not a problem.
So why does the solder paste turn black?Was it because of the poor operation during the solder paste printing process? The solder paste manufacturer sent skilled technicians on the same day.
After arriving at the customer's factory, the solder paste expert carefully observed each production step and found that the furnace temperature was not adjusted properly and the steel mesh was not cleaned thoroughly. After the adjustment, the problem of the solder paste turning black no longer occurred. The customer was very satisfied with the service of JJY and praised us. Not only was the quality of the solder paste products excellent, but the service was also very considerate. They expressed on the spot that they would always cooperate with us in the future. We are very glad to see that our customers are satisfied. Only by satisfying customers can we go further.
We will once again work in the same direction as the development trend of the electronic processing and manufacturing industry, uphold the spirit of craftsmanship, be meticulous and dedicated, and dare to innovate. We will persistently invest in high research and development, promote product upgrades, and bring professional, excellent and high-quality one-stop electronic soldering solutions to users in the field. With outstanding soldering products and a sense of responsibility, Contribute to the rise of China's electronic processing and manufacturing industry and make solder paste products and services better!
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account