The solder paste printing in the solder paste production process has gradually been given more attention. In the industry, it has also been widely recognized by many enterprises. Good arc welding requires products with long-term reliable quality. The printing of solder paste is quite popular. JJYSolder paste manufacturerTo analyze some problems that may occur during the production of solder paste.
Before application, the staff need to stir the solder paste with practical tools. The composition of the solder paste is also relatively uniform. When using a viscosity tester to test the viscosity of the solder paste, it is completed within the production and processing.
PrintingoneAfter a printed circuit board (or mechanical equipment calibration) is completed, it is neededSolder pasteThe detector conducts tests on solder paste, and it is necessary to inspect the top, bottom, left and right parts of the printed circuit board surface, etc., and record the relevant test values.
During the entire production and processing process, the quality of solder paste printing should be inspected. The inspection should be conducted on whether the patterns of the solder paste are detailed, whether the thickness is uniform, and whether there are any sharp edges on the solder paste, etc.
After the work is completed, the printed circuit board is processed in accordance with the requirements of the manufacturing processClean thoroughly. After the printing experiment or after the printing fails, the solder paste on the printed board should be cleaned with a cleaning machineCleaningAnd let it dry to prevent the formation of solder balls during reflow soldering caused by residual solder paste on the board when it is used again.
Shenzhen JJY brandOur solder paste is suitable for your choice. We offer a solution tailored to you. Solder paste,Solder wireFor solder rods and solder paste, choose JJY Solder Paste Manufacturer.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account