To meet the requirements of electronic manufacturers, solder paste producers have launchedNo-cleaning solder paste. However, in many high-precision scenarios, such as military and aerospace components of aircraft, even those with relatively weak activityRMASolder paste also needs to be cleaned to ensure its reliability. Even though it is highly active, it also brings about problems such as corrosion and leakage. Most electronic products can use no-rinse solder paste with very little residue.
Hazards caused by solder paste residues after soldering:
1Particulate pollutants are prone to cause electrical short circuits.
2Polar contaminants can cause dielectric breakdown, leakage and corrosion of component circuits, etc.
3The impact of non-polar contaminants on appearance is mainly due to the adhesion of white powder and dust, resulting in poor electrical contact.
The non-polar dirt mainly composed of rosin or other synthetic resins in the solder paste residue covers halogen, organic acids, salts, etc., playing a role of "plastic sealing", greatly reducing the corrosion of ionic dirt and avoiding leakage after absorbing moisture. During the cleaning process, the resin is washed away first. If the cleaning operation is stopped at this time, what remains on the circuit board will be ionic dirt. The consequences can be imagined. The problems caused by incomplete cleaning are far more serious than those of no cleaning at all. Therefore, once cleaning is carried out, it must be done thoroughly.
Shenzhen JJY Solder Paste Manufacturer has established mutually beneficial cooperation with electronic product manufacturers, providing fine electronic solder paste, solder wire, solder bar and other fine electronic solder products. It has a rich variety of successful cases in the research and development and application of fine electronic solder products. Relying on its overall strength, it has created a high-quality and honest sales market.
tags: JJY Lead-free solder paste Leaded solder paste Solder paste manufacturer Low-temperature solder wire Lead-free solder paste manufacturer
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account