High-temperature solder paste andLow-temperature solder pasteWhat's the difference? Questions that seem easy to answer are not easy to answer.JJYLet everyone know.
Low-temperature tincreamAs the name suggests, its melting point is relatively low. Its main components are tin and bismuth, with solder paste addedBIAfter that, the temperature will drop its melting point138℃. Applicable to components that cannot withstand high temperatures orPCBLow-temperature solder paste has relatively poor solderability, brittle solder joints and dull luster.
High-temperature solder paste has a relatively high requirement for temperature when passing through the furnace, and its melting point should be higher thanSN/BISolder paste, higher79℃The above main components are composed of tin, silver and copper, with a melting point of217℃-227℃That's all. It is widely used, has good weldability, is hard and firm, has good mechanical strength, and the weld points are bright.
JJYHigh-temperature solder pasteThe tin climbing effect is good and the service life is long. High activity, low porosity, and not prone to collapse; The solder joints are full and bright, with high strength and excellent electrical conductivity. Excellent printing performance and demolding performance, with fine pin spacing, mounting is effortless. It adopts imported flux and can be printed for a long time without affecting the wettability and viscosity of the solder paste.
Shenzhen JJY Industrial Technology Co., LTDHave12With years of experience in research and development and production, we have a strong technical force and stable product quality. JJY's factory is well-equipped, possesses proprietary technology and strictly implements itISO9001International Quality Management System Strict quality control, continuous stability, making customers worry-free, efficient, cost-effective and competitive! JJY welcomes you to call for consultation, inspection, sample request, purchase and use our products, and experience customized soldering solutions.
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account