Brand:JIAJINYUAN/JJY
Ingredients:One-component epoxy resin system
Product density1.32-1.34g/cm3
Product viscosity:300Pa.S - 320Pa.S
Color before curing:Bright red
Color after curing:Brown
Working temperature: 120/150℃
+86 0755 88366766
Red glue is used for SMD The electronic components are fixed PCB The adhesive on it (commonly known as: red glue). It is a one-component epoxy resin system that cures by heat, featuring excellent gluing performance, rapid curing upon heating, strong adhesion, resistance to repeated thermal shock from high-temperature soft solders, and a long shelf life. It is suitable for copper mesh, plastic mesh, double process and post-processing within a wide range of working environment temperatures AIIt meets the requirements of multiple lead-free wave soldering and other production processes, and maintains an extremely low drop rate.
The on-time delivery rate is as high as99%
This product is used for SMD The electronic components are fixed PCB The adhesive on it (commonly known as: red glue). It is a one-component epoxy resin system that cures by heat, featuring excellent gluing performance, rapid curing upon heating, strong adhesion, resistance to repeated thermal shock from high-temperature soft solders, and a long shelf life. This product is suitable for copper mesh, plastic mesh, double-process, and post-processing within a wide operating temperature range AIIt meets the requirements of multiple lead-free wave soldering and other production processes, and maintains an extremely low drop rate. ,
This product, red glue, must be used in advance2-3Take it out when it is small, seal it and let it thaw at room temperature. Do not heat it to warm up.DHS6688 Red glue is suitable for 22℃-28℃Use at room temperature. Do not add any solvents during use. The remaining red glue after use should be promptly recycled into a sealed container and placed in a container smaller than 6℃Store at a certain temperature. The remaining red glue after use and the unused ones Red glue must not be stored together.
Our experts tailor solder alloys, flux activity levels, cleaning methods, and specialty properties to your process. We optimize welding parameters and recommend application-specific solutions, boosting your first-pass yield.
5,000㎡ facility with ISO9001-certified and production & testing equipments. Full-process inspection: raw materials, processes, and finished products. SGS-certified eco-compliance: ROHS, REACH, ELV.
High-purity tin with lower dross rate than industry average. Fast wetting | Robust & glossy joints | Zero defects (cold joints, bridging, collapse,etc.). Factory-direct pricing for maximum cost efficiency.
Provide technical support: 24-hour response | 72-hour full resolution. Free material replacement & solder dross recycling. Pre-sales consultation & post-sales troubleshooting.
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.Founded in October 2008, is a collection of electronic solder R & D, production, customization, solutions, services in one of the customized solder solutions provider, “JIAJINYUAN” has been selected as a strong brand national demonstration project [solder materials]. Jiajinyuan factory covers an area of more than 5,000 square meters, with a number of modern production equipment, testing equipment and laboratory equipment. Our lead-free solder products have passed the “SGS” test and are fully compliant with the latest EU RoHS directive and REACH standard ....... If you have any questions, please feel free to contact us!
Service Hotline:+86 075588366766
Phone: +86 18938660310
Fax: +86 0755 88367866
QQ: 2790138382
Email: sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
National Service Hotline
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account