Product Name:Lead Free Solder Bar-Dip-Higher Temperature
Alloy:Sn96.5Ag3.5
Size(approx.):Trapezoidal Section(P18、Q25、H25)*L326 (MM)
Per Bar(approx.):1.105KG
Feature:Produced by pure tin and silver.Impurities are lowed to the minimum.
Application:For dip soldering process.
Packaging:Net weight 20KG/CTN
Shelf Life:2 Years
+86 0755 88366766
JJY Sn96.5/Ag3.5 is designed as a lead-free alternative for Sn/Pb alloys for electronics assembly operations.
JJY Sn96.5/Ag3.5 alloy has higher melting temperature than standard SAC alloys so may be used when high temperature assembly
is required.
The high silver content of JJY Sn96.5/Ag3.5 alloy contributes to stronger, shinier joints.
JJY Sn96.5/Ag3.5conforms and exceeds the impurity requirements of IPC-J-STD-006C and all other relevant international
standards.
For stabilization of copper, Cu content in the soldering pot(Sn-Ag-Cu), JJY Sn96.5Ag3.5 alloy will be recommended as a top up solder.
The on-time delivery rate is as high as99%
For dip soldering process with ROHS complianted.
Specification
SPECIFICATION
|
Item |
Specification |
|
Alloy Composition |
Sn96.5Ag3.5 |
|
Appearance |
Bright and shiny surface finishes |
|
Shape |
Bar |
|
Melting Point |
Approx. 221°C |
|
Density |
Approx. 7.5 g/cm³ |
|
Electrical Conductivity |
Approx. 14 %IACS |
|
Electrical Resistivity |
Approx. 12.3 μΩ.cm |
|
Soldering Temperature |
300-400°C |
|
Oxidation Resistance |
Good |
|
Amount of tin slag |
A small amount |
Our experts tailor solder alloys, flux activity levels, cleaning methods, and specialty properties to your process. We optimize welding parameters and recommend application-specific solutions, boosting your first-pass yield.
5,000㎡ facility with ISO9001-certified and production & testing equipments. Full-process inspection: raw materials, processes, and finished products. SGS-certified eco-compliance: ROHS, REACH, ELV.
High-purity tin with lower dross rate than industry average. Fast wetting | Robust & glossy joints | Zero defects (cold joints, bridging, collapse,etc.). Factory-direct pricing for maximum cost efficiency.
Provide technical support: 24-hour response | 72-hour full resolution. Free material replacement & solder dross recycling. Pre-sales consultation & post-sales troubleshooting.
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.Founded in October 2008, is a collection of electronic solder R & D, production, customization, solutions, services in one of the customized solder solutions provider, “JIAJINYUAN” has been selected as a strong brand national demonstration project [solder materials]. Jiajinyuan factory covers an area of more than 5,000 square meters, with a number of modern production equipment, testing equipment and laboratory equipment. Our lead-free solder products have passed the “SGS” test and are fully compliant with the latest EU RoHS directive and REACH standard ....... If you have any questions, please feel free to contact us!
Service Hotline:+86 075588366766
Phone: +86 18938660310
Fax: +86 0755 88367866
QQ: 2790138382
Email: sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
National Service Hotline
Tel:+86 0755 88366766
Phone:+86 18938660310
Email:sales@jjyhanxi.com
Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
Guangdong Public Security Backup 44030902002666 name
WeChat
WeChat official account