Recently, a customer inquired about the discovery during the welding processSolder pasteWhat should be done if the solder paste is too thin? Today, JJY Solder Paste Manufacturer will give you a simple analysis. If the solder paste is too thin, it may lead to the inability to obtain good solder joint quality during the soldering process.
The following are several possible temporary solutions to what to do if you find the solder paste is too thin:
1Stir and mix
Use a stirring rod or a dedicated solder paste mixer to thoroughly stir and mix the solder paste. This helps to evenly disperse the metal particles in it, making it more viscous.
2Refrigeration
Put the solder paste in the refrigerator or the chill compartment and chill it for a period of time. The low temperature can make the solder paste more viscous.
3Return it to the solder paste manufacturer for readjustment of viscosity.
The above is a simple analysis by JJY solder Paste Manufacturer on what to do if the solder paste is too thin during the soldering process. It should be noted that different solder paste brands and types may have different characteristics and usage requirements. Therefore, it is best to refer to the merchant's manual or contact better suggestions. In addition, to avoid affecting the soldering quality, it is recommended to conduct some small-scale experiments and tests before actual production operations to ensure that the adjusted solder paste meets the required viscosity and performance.