During the welding process, flux(flux)It helps and promotes the welding process, and at the same time has a protective effect on preventing oxidation reactions. Why use flux? Flux is used to join two metal surfaces. The connection is completed through fusion welding, hard brazing or soft brazing. The essence is basically the same, except that they are accomplished at different temperatures. The above three connection processes all use flux to remove oxides in order to form a strong bond between the bonding surfaces. The main difference between them lies in that welding and hard brazing do not require cleaning, but for electronic components, cleaning is a key process. After the connection process is completed, it is necessary to clean and remove the residues; otherwise, on-site failure will occur to a large extent. The specific situation depends on the components used and the type of flux.
The common metal surfaces connected by welding processes are copper and tin, both of which have a tendency to naturally oxidize. Therefore, in order to achieve their direct bonding, the oxides need to be removed. Flux can also perform some other functions at the welding temperature. They can reduce the surface tension of the solder, cause the solder to expand and promote wetting, thereby enabling the solder to form a strong and reliable solder joint.
It can also prevent the solder from further oxidizing during the welding process. To obtain additional oxidation protection, sometimes we also use nitrogen, but nitrogen does not play a role in the formation of intermetallic bonding, but it is indispensable for intermetallic bonding. In addition to its chemical properties, it also has excellent thermal stability, adhesion, ductility, electrolytic activity, environmental stability, chemical functional groups and their reaction properties, rheological properties, universal cleaning solutions and equipment adaptability, etc.
Want to know about solder pasteLead-free solder pasteFor any soldering issues such as solder paste, we welcome partners to consult Shenzhen JJY Industrial Technology Co., LTD. Let's learn and grow together! The solder wire, solder paste and solder rods of JJY brand are always waiting for partners to come and take them together.