inLead-free solder pasteAmong the product models,138℃The melting point of it is called low-temperature solder paste, and it is a kind of solder paste suitable for138℃At or above temperatures and with the use of low-temperature solder paste soldering process, low-temperature lead-free solder paste used in the soldering process is called low-temperature solder paste. To prevent components from and PCBThe plate can withstand high-temperature reflow soldering and is deeply resistant LEDFavor from the industry. The particle size of tin powder is25~45 umBetween them, the metal component is SnBi (sn42bi58)Now, let's talk about the characteristics from JJY solder Paste Manufacturer:
Lead-free low-temperature solder paste has the following characteristics:
(1Melting point138℃
(2It has good wettability and the weld points are bright, uniform and full
(3Solder beads and solder Bridges are produced during reflow soldering
(4It has a long bonding life and a long printing life of steel mesh
(5It is suitable for a wide range of process manufacturing and rapid printing
(6Excellent printability, eliminating omissions, depressions and fast formation during the printing process
The solder paste of Shenzhen JJY brand has gone through many years12Annual research and development of solder paste, solder wire, soldering wireLead-free solder pasteManufacturers of leaded solder paste, solder rods, leaded solder paste and other solder paste and wire products. Choose the solder paste manufacturer of JJY brand for solder paste