JJYLead-free solder pasteHow about it? What are the advantages and characteristics of its solder paste? With people's increasing emphasis and recognition of environmental protection, lead-free solder paste is increasingly favored in the production process. A lead-free surface can be regarded as one that contains no lead inside and is non-toxic to the human body. JJY lead-free solder paste is also very complete in variety, with different levels. You can follow me to take a look:
The product details are as follows:
FP-0M-305Lead-free high-temperature solder paste
Brand:JIAJINYUAN/JJY
Model:LFP-0M-305
Alloy composition:Sn96.5Ag0.3Cu0.5
Particle size:4#(20-38um)
Viscosity:200±20Pa.S
Activity: Weak activity
Melting point:217℃
Working temperature:235-250(℃)
Specification:500g/bottle
What are the features and advantages of lead-free high-temperature solder paste?
Lead high-temperature solder pasteLFP-0M-305It uses a special formulaRMAA uniform spherical lead-free solder paste with very little oxide contentSn96.5Ag3.0Cu0.5A uniform mixture of tin powder. This product has passedSGSTest compliantRoHSThe instructions contain solder paste that complies with the standards of the United StatesQQ-571As stipulated in itRMAType. This product strives to be highly compatible with the soldered product, with moderate wettability (activity), firm, bright and full solder joints, no solder beads, bridging, false soldering, less residue after soldering, high insulation resistance, good dry resistance, small viscosity change during continuous printing, ensuring the stability of long-term operation printing, good thixotropy and demolding property, good shape retention after printing, not easy to collapse, and components do not shift.
Solder paste has the characteristics of fast soldering, good moisture retention, no beads, prevention of dropping parts and prevention of stele erection. The tin powder particles used are small and uniform, and can be targeted0.2mmThe following is the extremely small spacing. in QFN,FPC,LEDIt is particularly outstanding in fields such asSMTSpecialized solder paste for surface mount printing can be adjusted according to the actual requirements of the customer. The solder paste produced by Double Chile Company is delivered on time. If you need it urgently, they will deliver it to your door as soon as possible. Their after-sales service is also first-class. If you use the solder paste from Double Chile, there will be detailed instructions for its use. The after-sales service will also patiently explain to you the precautions when using the solder paste. If you still have any questions, there will be professional engineers to explain them to you.
As mentioned above, leaded processing has better weldability than lead-free processing, but lead-free processing is more environmentally conscious. Want to know aboutSMTIn the patchSolder pasteFor other questions, partners are welcome to consult. Let's learn and grow together at Shenzhen JJY Industrial Technology Co., LTD.!