The solder paste formulas of various manufacturers in the soldering industry are different. Of course, different production processes will use different types of solder paste. Among them, lead-free solder paste is roughly divided into low-temperature solder paste, medium-temperature solder paste and high-temperature solder paste. The zero-halogen solder paste produced by JJY Solder Paste FactoryREACHLead-free high-temperature solder pasteLFP-JJY5RR-305T4AdoptSn96.5Ag3.0Cu0.5It is made of spherical solder powder of lead-free tin alloy with low oxidation degree, which has excellent environmental protection characteristics. At the same time, it is matched with a paste refined from imported chemical materials, which can achieve very high stability and effect. Below, the solder paste manufacturer will explain zero halogen andREACHCharacteristics of high-temperature lead-free solder paste:
1It has good demolding performance during printing, excellent dry resistance and good thixotropic performance, and can be applied to pad spacing≧0.3mmPrinting and fine spacingQFN,BGAThe mounting of devices.
2Zero halogen and compliantREACHIt is standard, with little and transparent residue after welding, non-corrosive, and has an extremely high insulation surface impedance value. It can achieve excellent performance without cleaningICTTest performance.
3When printing continuously, the viscosity change is small, which can ensure the stability of the printing effect during long-term operation.
4This product has excellent thixotropic performance and its form remains intact after printing,It is not easy to collapse and avoids the displacement of surface mount components.
5The weld points are bright after welding, with excellent electrical conductivity and gold-plated plates.QFNThe tin climbing has a high fullness.
6Fewer solder beads are produced during welding, reducing the occurrence of short circuits.
JJY solder Paste Manufacturer mainly engages in lead-free solder paste.SMTSurface mount solder pasteLEDResearch, development, production and supply of solder pastes, lead-free solder wires, wave soldering rods and other solder solders. For more knowledge about electronic soldering, please contact us. Welcome to interact with us.