How to choose a suitable solder paste in SMT assembly?

Headlines
inSMTIn surface mount processing, solder paste is widely used inPCBAAssemblyPCBAManufacturing and all kinds ofSMTIn the process, forPCBAThe quality of the finished product plays a decisive role. Solder paste is a kind of soldering material,…

News and information

Process control and manufacturing methods for lead-free solder paste - JJY Solder Paste Manufacturer

Process control and manufacturing methods for lead-free solder paste - JJY Solder Paste ManufacturerOct 14,2021

The process control and production methods when using lead-free solder paste. Nowadays, soldering of electronic products is an important production link. Currently, lead-free solder paste products are divided into low-temperature and high-temperature types, also known as leaded and lead-free. Each type has different production methods and controls. Now, let's first introduce the production method of high-temperature solder paste to you by the editor of the solder paste manufacturer: Semiconductor devices that operate at high temperatures, especially power devicesledPackaging, high-density integrated circuit packaging, and some precision......

Details >
What conditions are required for lead-free solder paste? How to use it? -- JJY Solder Paste Manufacturer

What conditions are required for lead-free solder paste? How to use it? -- JJY Solder Paste ManufacturerOct 13,2021

What conditions are required for lead-free solder paste? How to use it? During the production process of the electronics industry, solder paste is often discarded due to various reasons, and its price is relatively high. I think many industrial manufacturers are well aware of this. This aspect can also be utilized. After recycling and processing, it can be applied to industrial production, playing a role in reducing enterprise costs. Below, JJY Solder Paste Manufacturer will introduce to you some aspects and applications of lead-free solder paste: lead-free soldering......

Details >
What are the differences between lead-free solder paste and leaded solder paste? -- JJY Soldering Factory

What are the differences between lead-free solder paste and leaded solder paste? -- JJY Soldering FactoryOct 13,2021

What are the differences between lead-free solder paste and leaded solder paste? Generally speaking, the ingredients of solder paste are different, and so are their melting points. Nowadays, many products in society must have a combination of solder paste/Welding materials. In many industries, lead-free solder paste is mostly chosen to replace the previous leaded solder paste. This is because people's awareness of environmental protection is getting stronger and stronger. What are the differences between the two and how to distinguish them? Let's talk about it with JJY Factory: Leaded solder paste and lead-free solder paste have different colors.......

Details >
The application of lead-free solder paste in electronic products and how to choose high-quality solder paste?

The application of lead-free solder paste in electronic products and how to choose high-quality solder paste?Oct 12,2021

The application of lead-free solder paste in electronic products and how to choose high-quality solder paste? Nowadays, the pace of society is constantly advancing. Electronic devices such as mobile phones, computers, laptops, and smartwatches have become indispensable products in people's lives and work. These products are basically composed of circuit boards. Electronic components such as resistors, capacitors, diodes, and integrated circuits are closely combined with the circuit board through solder joints formed on the circuit board by solder paste. Realize the electrical connection function between components......

Details >
What does "no-clean" mean? What is no-clean solder wire? -- JJY Soldering Factory

What does "no-clean" mean? What is no-clean solder wire? -- JJY Soldering FactoryOct 12,2021

What does "no-clean" mean? What is no-clean solder wire? At present, the no-clean soldering process is increasingly widely applied in related fields of the electronics industry. As a supporting process material product for lead-free tin wire, it has also been continuously developed and improved. To ensure that electronic equipment is not cleaned after soldering, soldering has high equivalence and reliability. Now, let's have a look at it with the help of the editor from JJY:What does "no cleaning" mean? After soldering with ordinary solder wire, there is a lot of rosin residue at the edge of the solder joint......

Details >

contact

  • Tel:+86 0755 88366766
  • Phone:+86 18938660310
  • Email:sales@jjyhanxi.com
  • Address:13/F,12/F, Building No. B,Qinghu Technology Park,Qingxiang Rd.,Qinghu Community, Longhua Subdistrict,Longhua District,Shenzhen City,GUANGDONG Province,P.R.C.(518027)
  • Guangdong Public Security Backup 44030902002666 name
  • JJY TIN SOLDERWeChat
  • JJY TIN SOLDERWeChat official account
SHENZHEN JIAJINYUAN INDUSTRIAL TECHNOLOGY CO., LTD.@All rights reserved. Low temperature tin wire, lead-free solder paste, lead solder paste